Three different biological systems, the consortium of autotrophic bacteria Acidithiobacillus ferrooxidans and Acidithiobacillus thiooxidans, heterotrophic fungus Aspergillus niger and heterotrophic yeast Rhodotorula mucilaginosa, were investigated for lithium extraction from lepidolite. The bacterial consortium was the most effective, 11 mg l−1 of Li was dissolved in the absence of nutrients within 336 days. Fungal and yeast bioleaching was faster (40 days), however, with lower extraction efficiency. Bioaccumulation represented a main process of Li extraction by R. mucilaginosa and A. niger, with 92 and 77% of total extracted Li accumulated in the biomass, respectively. The X-ray diffraction analysis for bioleaching residue indicated changes caused by microorganisms, however, with differences between bacterial leaching and bioleaching by fungi or yeasts. The final bioleaching yields for bacterial consortium, A. niger and R. mucilaginosa were 8.8%, 0.2% and 1.1%, respectively. Two-step bioleaching using heterotrophic organisms followed by autotrophic bioleaching could lead to the increase of the process kinetics and efficiency. Bioaccumulation of Li offers strong advantage in Li extraction from solution.
This study describes the water vapour effect on the oxidation resistance of 9Cr creep resistant steels. Boiler P91 and MarBN steels were oxidized for 3000 h in a simulated humid atmosphere with ~10% water vapour. The oxidation kinetics had a stable course for 1000 h and was evaluated by the weight gain curves for both experimental steels and both oxidation temperatures. The oxidation rate was higher at 650 °C versus 600 °C, as reflected by the oxidation rate coefficient. A significant increase occurred after 1000 h of oxidation, which was related to the local breakdown oxide scale and oxide nodules were formed on steel. This oxidation behavior was influenced by the fact that a compact spinel structure of iron oxides and alloying elements were not formed on the steel. Analysis after 3000 h of exposure showed hematite Fe2O3 formed on the outer layer, magnetite Fe3O4 on the middle layer, and the bottom layer consisted of iron-chromium-spinel (Fe,Cr)2O3.
Influence of SPD process realized by ECAP on structural formation and mechanical properties was searched. Samples after ECAP were heat treated at various temperature and time conditions. Investigation material bases were high purity aluminium and aluminium alloys EN AW 6082, EN AW 2014. The best material properties are describing in dependence on experimental conditions.
The effect of heat treatment on microstructure and mechanical properties of extruded SiC/6061 aluminium alloy matrix composite was investigated. The heat treatment (annealing at 540 °C for 1.5 hours, water quenching and artificial aging at 170 °C for 7 hours) caused dissolution of Mg2Si particles and decomposition of small SiC particles. The 0.2 % yield strength and the ultimate tensile strength of extruded composite were increased by application of heat treatment due to precipitation of β´´ phase particles. On the other hand, the ductility of composite was decreased. The fracture surface of as-extruded composite was consisted of numerous dimples. It was a result of micro voids nucleation at interface between matrix and SiC particles and second-phase particles. The fracture of heat treated composite was similar, micro voids were nucleated mainly on SiC particles, which were cracked during tensile test.