In this work, sugarcane bagasse fiber, a waste product of agroindustry, was added to mortar mixes at different proportions looking to seal porosities so as to improve the resistance of concrete to carbonation and to improve its mechanical properties. To evaluate the behavior of bagasse fibers in the alkaline media typical of mortars, bagasse fibers were subjected to solutions with alkaline pH values, and their chemical structure and morphological behavior was evaluated using FTIR (Fourier transform infrared spectroscopy) and SEM (Scanning Electron Microscopy). Using mortar cylinders in an accelerated carbonation chamber to obtain results in short lapses, the compressive strength and the carbonation were evaluated. The FTIR analysis results indicate that pH values of 11 and 12 causes a delignification, while at pH 9 and 10, a swelling of the molecule occurs because of the addition of hydroxyl ions, behavior that is confirmed with SEM images. A clear effect of the fiber addition on the performance of concrete was observed as the carbonation front of 35 mm for the sample without fibers was reduced to 2 mm for the sample with 2% fiber addition, resulting in an increase of 5 MPa in compressive strength. These results indicate that in the range of mortar pH, chemical changes occured over the sugarcane surface that could cause the growth of fibers and could partially seal the porosity in the mortars, thus enhancing its performance.
Fue evaluado el efecto de realcalinización electroquímica aplicando las normas UNE-EN-1504, NACE-SP0107 2007 y NMX-C-553-ONNCCE-2018, en muestras de concreto reforzado previamente carbonatadas. Con el seguimiento del grado de realcalinización, mediante mediciones de pH y potencial de media celda a 7, 14, 21 y 28 días, se observa la recuperación del pH en todos los casos, obteniendo valores de potencial de media celda característicos en cada aplicación de corriente, que confirma la polarización del acero modificando la condición termodinámica de la intercara concreto-acero y ocasionando cambios químicos en la pasta de concreto. Con la norma NMX-C-553-ONNCCE-2018 se polarizó el acero sin llegar a la región de sobreprotección, evitando el riesgo de producir hidrógeno y fragilidad en el acero
The properties of rock aggregates in Seybaplaya, Campeche, Mexico were analyzed, highlighting their uniaxial compressive strength [8.6 - 84.7 MPa], moisture content [3.73 - 13.62 %], real density [1.9 - 2.615 g/cm³], specific weight [18.71 - 25.65 kN/m³], porosity [9.73 - 28.45 %], and rebound value [19 - 45 J], emphasizing the importance of these properties for the design and construction of masonry structures.
In this study, waste materials such as recycled glass employed to synthesize mesoporous silica nanoparticles (NPs) and/or sugarcane bagasse fiber (SBF) were used to reinforce concrete samples, and their properties were evaluated. The cement additions used in this study were 0.8% NPs (0.8N), 1% SBF (1F), or a combination of the two (0.8N-1F). The addition of 0.8N-1F slightly improved the mechanical performance of concrete and offered the greatest decrease in carbonation, likely because these materials had the fewest permeable voids. The thermodynamic properties at the concrete‒steel interface tended to be reduced when the components were added, and there were marked differences in the corrosion potential and corrosion kinetics in concrete with the addition of SBF and NPs. Each material enhanced the performance properties of concrete, but the combination of both materials had a positive synergistic effect on all the studied properties.
Se diseñó y construyó una Cámara de Carbonatación Acelerada (CCA) con una capacidad de 70 muestras de 15 cm de sección por 30 de largo, capaz de mantener condiciones controladas de CO2 (4 % ± 0.5 %), y humedad relativa (65 % ± 5 %), con el objetivo de acelerar el proceso de carbonatación de muestras de concreto armado y facilitar estudios sobre la pérdida de pasivación del acero y el proceso de corrosión. La validación de la CCA se determinó mediante la profundidad de carbonatación por el método de vía húmeda utilizando indicadores ácido-base (timolftaleína y fenolftaleína) en muestras testigo sin acero, alcanzando una profundidad de carbonatación de hasta 7.0 cm en un periodo de seis meses.