Stearic acid (SA) is being used as phase change material (PCM) in energy storage applications. In the present study, the microencapsulation of SA with SiO2shell was carried out by sol–gel method. Different amounts of SA (5, 10, 15, 20, 30 and 50 g) were taken against 10 ml of tetraethyl orthosilicate (TEOS) for encapsulation. The synthesized microencapsulated PCM (MEPCM) were characterized by Fourier transform infrared spectroscope (FT-IR), X-Ray diffraction (XRD), X-Ray photoelectron spectroscopy (XPS) and scanning electron microscopy (SEM). The characterization results showed that SA was successfully encapsulated by SiO2. Thermogravimetric analysis (TGA) exhibited better thermal stability of the MEPCM than SA. The enthalpy values of MEPCM were found to be unchanged even after 30 heating–cooling cycles by differential scanning calorimetry (DSC). The latent heats of melting and solidification of 50 g SA containing MEPCM were found to be highest i.e. 182.53 J/g and 160.12 J/g, respectively among all microencapsulated samples. The encapsulation efficiency values were calculated using thermal data and the efficiency was found to be highest i.e. 86.68% in the same sample.
Steel structures significantly degrades owing to corrosion especially in coastal and industrial areas where significant amounts of aggressive ions are present. Therefore, anodic metals such as Al and Zn are used to protect steel. In the present study, we provide insights for the corrosion mechanism and kinetics of Al-Zn pseudo alloy coating deposited on mild steel plate via an arc thermal spraying process in 3.5 wt.% NaCl solution in terms of its improved corrosion resistance properties at prolonged exposure durations. Electrochemical studies including open circuit potential (OCP) and electrochemical impedance spectroscopy (EIS) on the deposited coating at longer exposure durations revealed enhanced corrosion resistance properties while the morphology of corrosion products through field emission-scanning electron microscopy (FE-SEM) indicated their compactness and adherence. Furthermore, atomic force microscopy (AFM) confirmed reduced roughness when compared with that of unexposed coating. Additionally, X-ray diffraction (XRD) and Raman spectroscopy results confirmed the formation of protective, adherent, and sparingly soluble Simonkolleite (Zn5(OH)8Cl2.H2O) after 55 d of exposure in 3.5 wt.% NaCl solution. A schematic is proposed that explains the corrosion process of Al–Zn pseudo alloy coating in 3.5 wt.% NaCl solution from the deposition of coating and initiation of corrosion to longer exposure durations.
We report the production of an efficient anti-corrosive coating of cold-rolled (CR) steel in a seawater environment (∼3.5 wt% NaCl aqueous solution) using an oil-based graphene oxide ink. The graphene oxide was produced by heating Aeschynomene aspera plant as a carbon source at 1600 °C in an argon atmosphere. The ink was prepared by cup-milling the mixture of graphene oxide and sunflower oil for 10 min. The coating of ink on the CR steel was made using the dip-coating method, followed by curing at 350 °C for 10 min in air atmosphere. The results of the potentiodynamic polarization show that the corrosion rate of bare CR steel decreases nearly 10 000-fold by the ink coating. Furthermore, the salt spray test results show that the red rusting in the ink-coated CR steel is initiated after 100 h, in contrast to 24 h and 6 h in the case of oil-coated and bare CR steel, respectively. The significant decrease in the corrosion rate by the ink-coating is discussed based on the impermeability of graphene oxide to the corrosive ions.