This study was observed the effect of cleansing agents and adhesive resins on shear bond strength (SBS), surface morphology and phase transformation of saliva and silicone disclosing medium contaminated zirconia. The 110 zirconia specimens size 5×5×1mm were fabricated and randomly divided into 5 surface treated groups: Non-contaminated (PC) Saliva and silicone disclosing medium contaminated without cleansing (NC) Surface contaminated and cleansing with Phosphoric acid (PO) Ivoclean (IC) or Hydrofluoric acid (HF). The twenty of each surface treated specimens were selected and bonded with Panavia F2.0 (P) and Superbond C&B (S) for SBS test (n=10). The data was analyzed by Kruskal-Wallis H and Mann-Whitney U test. The remaining specimens of each surface treated groups were examined by SEM and XRD. The saliva and silicone disclosing medium contaminated zirconia without cleansing group (PNC) had the lowest SBS when Panavia F2.0 was used for cementation (p0.05). However, there were no difference in SBS among groups when cementation with Superbond C&B (SPC, SNC, SPO, SIC and SHF) (p>0.05). There was no morphologic changing that could be observed by SEM. The XRD showed little phase transformation when surfaces were contaminated and cleaned. The saliva and silicone disclosing medium contaminated zirconia should be cleaned with Phosphoric acid, Ivoclean or Hydrofluoric acid for 20s prior to cementation with Panavia F2.0. However, the surface cleansing was not necessary when cementation with Superbond C&B.
The residual monomer remaining in acrylic resin can cause an allergic reaction and is toxic to oral soft tissue. This study determined the effect of the duration of ultrasonic cleaning on the amount of residual methyl methacrylate monomer in one heat-polymerized acrylic resin, Meliodent, and three autopolymerized acrylic resins, Unifast Trad Ivory, Unifast Trad Pink, and Unifast III. Thirty-six disc-shaped specimens of each brand were prepared and randomly divided into six groups: control (no treatment), positive control, and ultrasonic treatment in 50°C water for 3 minutes, 5 minutes, 10 minutes, or 15 minutes. The residual monomer was extracted and analyzed using high performance liquid chromatography. There were no significant differences in the residual monomer amount in the Meliodent groups. The amounts of residual monomer in the autopolymerized acrylic resin positive control group and ultrasonic treatment groups were significantly lower than those of the control group for the Unifast Trad Ivory, Unifast Trad Pink, and Unifast III groups (P < 0.05). The amount of residual monomer was not significantly different between the ultrasonic treatment in 50°C water (3 minutes for Unifast Trad Pink and 5 minutes for Unifast Trad Ivory and Unifast III) groups and the positive control group (P > 0.05). Ultrasonic treatment with 50°C water for 3-5 minutes for autopolymerized resin and 3 minutes for heat-polymerized acrylic resin reduced the amount of residual monomer similarly to previously recommended methods, using shorter treatment times.
10 August 2021 in International Journal of Dentistry
Background and Purpose. Contamination of the lithium disilicate (LDS) during the try-in procedure is unavoidable and may weaken the bond strength of restoration. The purpose of this study was to investigate the efficacy of different surface cleansing agents on the shear bond strength (SBS) of contaminated LDS. Materials and Methods. Seventy LDS specimens were randomly divided into seven groups. The first group was noncontaminated surface (PC). The six other groups were contaminated with the saliva and silicone disclosing medium and treated with no surface cleansing agent (NC); phosphoric acid (PO); Ivoclean (IV); sodium hydroxide solution (NA); Restorative Cleansing Agent (RC); and hydrofluoric acid (HF). Then, LDS specimens were cementated with Panavia V5 to resin composite rod. Each specimen was subjected to an SBS test. The modes of failure was inspected under light microscope. The surface element of each group was examined by SEM-EDS. Results. The results were analyzed with one-way ANOVA and Tamhane’s T2. The mean SBS value of NC was significantly lower than others ( ), and HF was significantly higher than others ( ). However, PC, PO, IV, NA, and RC were not significantly different from each other ( ). The mode of failure was mostly adhesive failure in every group. The surface showed similar amount of elements in every group. Conclusions. The SBS of LDS was reduced by saliva and silicone disclosing medium contamination which can be restored using acid- and alkaline-based surface cleansing agents before the cementation procedure.
The scanned abutment file for the digital design of restorations can be either obtained directly using the intraoral scanner (IOS) or scanning the impression or the working model with the extraoral scanner (EOS). The trueness of the scanned file pertains to its effect on the accuracy of the restoration. Objective This study aimed to compare the trueness of scan files from different intraoral scanners (IOSs) and the hybrid workflow using the E3 extraoral scanner (EOS) for ceramic restoration. Methodology The model of the mandibular right first molar was prepared for the ceramic crown, and it was scanned with the EOS in reference Standard Tessellation Language (STL) file format. The following seven experimental groups were investigated. The IOSs—iTero Element 5D (IT), Trios 4 (TF), Medit i700 (MI), Primescan (PM), Virtuo Vivo (VV)—were directly scanned on the prepared model. The silicone impression of the prepared model was scanned with EOS (IS). The working model poured from the impression was scanned with the EOS (WS). The test STL file was trimmed and superimposed on the reference STL file for the trueness assessment using Geomagic Control X. The point deviation at the surface and margin of each group were compared. The mean deviation was calculated and statistically analyzed with One-way ANOVA (α=0.05). The minimum and maximum deviation of each area were also recorded. Results Compared with the other groups, the impression scan group had a significantly greatest deviation (p<0.05) in surface (37.65±1.14 µm), margin (63.57±5.85 µm) and overall (50.61±3.28 µm). The WS group showed significantly greater deviation (p<0.05) in surface (23.93±1.20 µm), margin (46.18±2.00 µm) and overall (35.05±1.16 µm) than the IOS groups. In some IOS groups, the deviation was also significantly different (p<0.05). Conclusion The IOS is recommended for obtaining the scanned file due to its lesser deviation when compared to the hybrid workflow. While statistical differences exist among IOSs, the clinical relevance of these differences appears minimal. If the IOS does not exist, scanning the working model is preferred over scanning impressions directly. However, further clinical validation studies are necessary to confirm this finding.
1 November 2019 in Journal of Physics: Conference Series
Nowadays, titanium alloy is widely used as orthodontic mini-screw implants due to its suitable mechanical properties and excellence in biocompatibility. However, the excessive torques applied during the insertion of orthodontic mini-screw implant can cause necrosis of the surrounding bone. In this article, the insertion torque of orthodontic mini-screw implants is aimed to reduce during treatment by means of surface coating. The three types of coatings, namely, DLC, F-DLC 2:1 and Si-DLC 2:1 coated on orthodontic mini-screw implants were chosen to take into account the insertion torque values compared with uncoated surface. The friction behaviors of the films in ambient air and dry air were assessed using ball-on-disk friction testing. Cytotoxicity tests were performed using MTT assay. The insertion torque values were measured by physiodispenser. The results indicated that, both measured in ambient air and dry air, the addition of F into the DLC films slightly influenced the friction coefficients, while doping with Si strongly influenced the films. These films also exhibited less cytotoxicity on their surfaces. Furthermore, the insertion torque values decreased when coated orthodontic mini-screw implants with F-DLC 2:1 and Si-DLC 2:1 films. Therefore, the F-DLC 2:1 and Si-DLC 2:1 films can be considered to apply on orthodontic mini-screw implant for reducing the insertion torque.
About Me
Taksid Charassenagpaisarn received his Ph.D. in Dental Biomaterials Science from Chulalongkorn University. He works as an Assistant Professor at Rangsit University. His research interests mainly include: dental biomaterials, dental materials, digital dentistry, implant dentistry, prosthodontics, and restorative dentistry.
Taksid Charassenagpaisarn received his Ph.D. in Dental Biomaterials Science from Chulalongkorn University. He works as an Assistant Professor at Rangsit University. His research interests mainly include: dental biomaterials, dental materials, digital dentistry, implant dentistry, prosthodontics, and restorative dentistry.