Mohamed Gebril

Prof. Dr. Mohamed Gebril

Department of Mechanical Engineering, University of Benghazi, Benghazi, Banghāzī, Libya
University of Benghazi, Faculty of Engineering, Mechanical E...

Research Focus & Metrics

Academic Career Length

17Years (2010-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
27 January 2023 in Materials
Verified
Journal Article
Open access
PDF file
MGMohamed Gebril
Mohamed Gebril
MOMohd Zaidi Omar
Mohd Zaidi Omar
IMIntan Fadhlina Mohamed
Intan Fadhlina Mohamed
NONorinsan Kamil Othman
Norinsan Kamil Othman
DEDawod Mohamed Elabar
Dawod Mohamed Elabar
OIOsama Irfan
Osama Irfan
Improving the engineering properties of Al–7Si cast alloys (300 series) provides an attractive alternative to automotive and aircraft engine industries. The solubility limit of silicon (Si) in Al contributes to the precipitation of flake-shaped Si particles with sharp edges, which function as a stress riser and promote crack propagation during the eutectic phase while also weakening the protective layer’s durability. In this study, the impact of microstructure refinement of Al–7Si alloys by using cooling slope, thixoforming and the T6 heat treatment process on hardness and corrosion resistance behavior was investigated. Results showed that the microstructures of the as-cast alloy had a very coarse dendritic shape, whereas the dendritic transferred to the globular α-Al phase, and the Si particles were replaced into a lamellar- or acicular-like shape after the cooling slope and thixoforming process, respectively. The as-cast, cooling slope and thixoformed samples were subjected to the T6 heat treatment process, which enhanced the hardness to 79, 99 and 104 HV, respectively, due to Si particle refinement. The potentiodynamic test revealed that the corrosion rate dropped to 0.00790 and 0.00736 mmpy−1 in the heat-treated cooling slope and thixoforming samples. This finding can be attributed to the substantially refined Si particles and reduced eutectic phase area due to the smaller cathodic to anodic area ratio.

8 March 2019 in Metals
Verified
Journal Article
Open access
PDF file
MGMohamed Gebril
Mohamed Gebril
MOMohd Zaidi Omar
Mohd Zaidi Omar
IMIntan Fadhlina Mohamed
Intan Fadhlina Mohamed
NONorinsan Kamil Othman
Norinsan Kamil Othman
As-cast and semisolid casting using a cooling slope A356 alloy were processed by equal channel angular pressing (ECAP) for Si and grain refinement. The ECAP was conducted at room temperature in a mold, with a channel angle of 120°, and this resulted in a significant size reduction of grain and Si particles from 170.5 and 4.22 to 23.12 and 0.71 µm, respectively, after six passes of heat-treated cooling slope casting, using the ECAP process. The hardness increased with ECAP processing, from 61 HV, for the as-cast alloy, to 134 Hv, after six passes of heat-treated cooling slope casting. The corrosion resistance of the alloy improved, from 0.042 to 0.0012 mmy−1, after the ECAP process. In this work both the strength and corrosion resistance of the ECAPed A356 alloys were improved with the application of the cooling slope process than without (i.e., from the as-cast condition).

17 May 2022 in Metals
Verified
Journal Article
Open access
PDF file
MGMohamed Gebril
Mohamed Gebril
MOMohd Zaidi Omar
Mohd Zaidi Omar
IMIntan Fadhlina Mohamed
Intan Fadhlina Mohamed
NONorinsan Kamil Othman
Norinsan Kamil Othman
OIOsama Irfan
Osama Irfan
A356 aluminium alloy is subjected to heat treatment and high-pressure torsion (HPT) processing to investigate the impact of the combined treatments on the alloy’s microstructure refinement, corrosion resistance and hardness. The high-pressure torsion process was performed at room temperature for 0.75 and 5 turns. Subjecting the A356 Al alloy to a heat treatment and subsequent HPT processing produced a more refined microstructure, which has the effect of enhancing the alloy hardness and corrosion resistance under fragmentation and the homogenous redistribution of the intermetallic compounds and the Si particles. The results of the treatment show that there is a marked increase in hardness when imposing a strain from 61 HV to 198 HV on the A356 Al alloy, which has been HPTed and heat-treated for five turns. The polarisation curves show that there is a considerable improvement in the corrosion resistance rate of the alloy from 0.043 mm·year−1 for the A356 Al alloy sample to 0.003 mm·year−1 after five turns of HPT. In this work, the microstructure refinement resulted in the improvement of both the mechanical strength and corrosion resistance of the aluminium 356 alloy after heat treatment in comparison to the untreated alloy.

2 November 2023 in Metals
Verified
Journal Article
Open access
PDF file
MGMohamed Gebril
Mohamed Gebril
MOMohd Zaidi Omar
Mohd Zaidi Omar
IMIntan Fadhlina Mohamed
Intan Fadhlina Mohamed
NONorinsan Kamil Othman
Norinsan Kamil Othman
AAAhmad Muhammad Aziz
Ahmad Muhammad Aziz
OIOsama Irfan
Osama Irfan
Improving the engineering properties of A356 alloy is an appealing option for the automotive industry. This study aimed at refining and redistributing Si particles and the eutectic phase by applying T6 heat treatment to a semi-solid A356 alloy, followed by severe plastic deformation (SPD). Using a cooling-slope technique, the as-cast and rheocast samples were subjected to heat treatment prior to being processed using equal-channel angular pressing (ECAP) and high-pressure torsion (HPT) at room temperature. The results show that the brittle Si particles were effectively fragmented and redistributed in the homogenous microstructure. The grain size reduced from 170 μm to 23 μm in the as-cast sample after combining heat treatment and the cooling-slope. This was followed by the ECAP sample after six passes through route A (where the sample is not rotated between each pass), while it reduced to 160 nm after five turns of the HPT process in a heat-treated cooling-slope sample. The hardness of the heat-treated cooling-slope casting samples increased with the ECAP process; there was an increase from 61 HV to 134 HV for the as-cast alloy after six passes through route A. The hardness of the heat-treated cooling-slope sample improved with the HPT process to 211 HV after five turns.

31 December 2019 in Sains Malaysiana
Verified
Journal Article
Closed access
MGMohamed Gebril
Mohamed Gebril
MOMohd Zaidi Omar
Mohd Zaidi Omar
NONorinsan Kamil Othman
Norinsan Kamil Othman
IMI.F. Mohamed
I.F. Mohamed

1 April 2013 in Advanced Materials Research
Verified
Journal Article
Closed access
PDF file
MGMohamed Gebril
Mohamed Gebril
Mohammed AldlemyMohammed Aldlemy
Mohammed Aldlemy
AKAbdessalam F. Kablan
Abdessalam F. Kablan
The tempering process of medium and high carbon steel using quenching in water as quenching medium with different tempering temperatures has been investigated. The samples were quenched to room temperature in water. The mechanical properties and corrosion rate of the quench and tempering samples were measured. The result shows that hardness value of the medium and high carbon steel increased due to formation of martensite structure which is very strong phase but it is normally very brittle, so it is necessary to modify the mechanical properties and relieve internal stresses by heat treatment in the range 100-700°C. The experimental results revealed that mechanical properties of selective alloy were significantly changed by temper treatment. By increasing the tempering temperature, hardness and ultimate tensile strength are gradually decreased and ductility was improved. Moreover, the corrosion rate has been studied and shown within multiple phase structure corrosion rate increased more than martensite structure even its stressed structure.