This paper is a contribution to the theoretical and quantitative understanding of the processes for the production of magnesium metal by metallothermic process in vacuum (Pidgeon Process). In the present study, effects of reductant type and amount were investigated. CaC 2 is a low-cost alternative to FeSi (ferrosilicon) which is the common reductant in the Pidgeon Process. CaC 2 slightly decreases the Mg recovery ratios but it remarkably decreases the process cost. The experimental study, conducted with the change of mass % FeSi–CaC 2 ratio at 1,250 °C for 360 min, the optimum Mg recovery was measured as 94.7 % at 20 % CaC 2 addition. Also aluminum, as a reductant, allows conducting the process at lower temperatures than that of FeSi. For the experiments conducted with Al addition, the highest Mg recovery ratio was measured as 88.0 % in the conditions for 300 min process duration and 100 % stoichiometric Al addition at 1,200 °C.
1 April 2014 in High Temperature Materials and Processes
Self-propagating high temperature synthesis (SHS) is a very important technique for the synthesis of high technology ceramics, metals and alloys. SHS parameters of TiB 2 were carried out in this study. Mg stoichiometry as reductant, process atmosphere and addition of NaCl and MgSO 4 ·7H 2 O additives were investigated. HCl leaching was applied to SHS products to purify their TiB 2 contents. Stoichiometrically 100% Mg addition ratio and Ar atmosphere were determined as the optimum parameters. NaCl addition was also positively affected the specific surface area values. 11.78 m 2 /g specific surface area value was measured for 5.0% NaCl addition ratio.
21 July 2018 in High Temperature Materials and Processes
Mill scale (MS) has a potential to use as an iron source because of its high iron content. MS mainly consists of a mixture of iron oxides, metallic iron and other base metal oxides. MS is formed on the surfaces of steel ingots during continuous casting as a waste material. In this study, the use of MS as an iron source for the production of carbon-free iron containing alloys (unalloyed iron, Fe-Ni, Fe-Cr-Ni, Fe-Cr-Ni-Mo) via a metallothermic reduction process was investigated. Thermodynamic calculations and the experimental studies were performed on the basis of 100 g of MS. The effects of different stoichiometric amounts of MS and aluminum (Al) powders (as reductant) were investigated for the production of unalloyed Fe. While, different amount of metal oxide ratios and their effects on metal recoveries, compositions and microstructure of final alloys were studied during Fe-based alloys production. The highest iron recovery during unalloyed Fe production was obtained as 95.14 % by using 100 g of MS and 100 % stoichiometric Al (28.6 g) containing mixture. In Fe-based alloys production series, the highest metal recovery values were reached up to 95.0 % for Fe, 95.1 % for Ni, 68.3 % for Cr and 77.2 % for Mo, respectively.
26 October 2020 in Mining, Metallurgy & Exploration