Moisture ingress into PV module in the presence of ultraviolet radiation, high temperature, and other environmental stressors can affect the optical integrity of the PV module. Optical degradation can take the form of delamination, discolouration of encapsulant, metal grids corrosion, and trapped moisture or chemical species. This can influence the photon absorption and current transport properties in the PV module bulk, which can affect the module operating temperature. In the present work, the relationship between optical degradation and temperature sensitivity of 20-year-old multicrystalline silicon field-aged PV modules have been investigated. The selected PV modules were characterized using visual inspection, current-voltage (I–V) characterization, temperature coefficients profiling, current resistivity profiling, infrared (IR) thermal, ultraviolet fluorescence (UV–F), and electroluminescence (EL) imaging. PV modules affected by optical degradation show weak fluorescence and luminescence signal intensities. The average difference in cell temperature (ΔT) between the warmest and coldest cell for the PV modules investigated was found to be around 10 ± 2 °C and the average power degradation rate was approximately 0.8% per year. The underlying factor for the observed degradation is attributed to the degradation in the temperature coefficients of open circuit voltage (βVoc) and maximum power point voltage (βVmpp). The average temperature coefficient of efficiency (βηm) of the modules was found to be around −0.5%/°C. Finally, a temperature dependent resistivity method for extracting temperature coefficients from IR thermal data of PV modules has been proposed.
One effect of moisture ingress on solar panels is potential induced degradation (PID). Solar panels affected by PID experience large leakage currents between the solar cells and the module’s frame, which leads to substantial power degradation. In the present work, the temperature coefficients of 3 old PV panels affected by PID were investigated. In the electroluminescence images, solar cells nearer to the edge of the modules appear darker due to ohmic shunting. IR thermal images acquired under clear sky outdoor conditions show that the majority of the warmer cells (hotspots) were located closer to the edge of the modules. The difference in cell temperature (∆T) due to PID effect ranges from 7 °C to 15 °C for the 3 field-aged modules. The average temperature coefficient of efficiency (βηm) was found to be −0.5%/°C. Also, it was observed that the temperature coefficients of open circuit voltage (βVoc = −0.4%/°C), maximum power point voltage (βVmpp = −0.5%/°C), and fill factor (βFF = −0.2%/°C), were the underlying factors for the degradation in the Pmax of the old solar panels affected by PID. This accounted for an average 1.2%/year overall degradation in the efficiency of these modules. Most notably, it was discovered that the PV modules affected by PID show negative temperature coefficients of maximum power point current (βJmpp) due to large leakage currents. This observed negative βJmpp we believe is characteristic of PV panels affected by PID.