The effect of proton irradiation on the structure, phase composition, defect state and nanohardness of Zr/Nb nanoscale multilayer coatings was investigated. Preservation of the Zr/Nb layered structure with 50 and 100 nm thick layers, was observed after irradiation with protons at 1720 keV energy and 3.4 × 1015, 8.6 × 1015 and 3.4 × 1016 ions/cm2 fluences, and the interfaces remained incoherent. In the Zr/Nb nanoscale multilayer coatings with individual layer thicknesses of 10 and 25 nm, there were insignificant fluctuations in interplanar distance, which were influenced by changes in irradiation fluence, and the interfaces were partially destroyed and became semicoherent. Changing irradiation fluence in the investigated ranges led to a decrease in the nanohardness of the Zr/Nb nanoscale multilayer coatings with individual layer thicknesses of 10–50 nm. Variable-energy positron Doppler broadening analysis revealed that these changes are primarily caused by peculiarities of the localization and accumulation of the embedded ions and do not cause a significant increase in the S-parameters of Zr/Nb nanoscale multilayer coatings with a layer thickness less than 100 nm.
17 April 2024 in Journal of Vacuum Science & Technology B
Effects of postgrowth high-temperature annealing on vacancy complexes and photoluminescence (PL) from GeSiSn/Si multiple quantum wells (MQWs) are studied. The series of PL peaks related to the vacancy-tin complexes was observed for as-grown samples including different structures, such as GeSiSn/Si MQWs, multilayer periodic structure with GeSiSn quantum dots (QDs), GeSn cross-structures upon GeSiSn/Si MQWs, and thick GeSiSn layers. The PL band intensity is significantly reduced after annealing at 700 °C corresponding to the reduction in vacancy density, as demonstrated by the positron annihilation spectroscopy (PAS) data. Such annealing also results in the appearance of the PL signal related to the interband optical transitions in GeSiSn/Si MQWs. However, the high temperature could negatively impact the sharpness of heterointerfaces due to Sn diffusion, thus limiting the PL efficiency. To improve the luminescence properties of GeSiSn/Si structures, we proposed a two-stage technique combining both the annealing and subsequent treatment of samples in a hydrogen plasma at 200 °C. The plasma treatment significantly reduces the PL band of vacancy-related defects, whereas annealing at a moderate temperature of ∼600 °C prevents the blurring of heterointerfaces. As a result, we demonstrate an increase in the relative efficiency of interband PL of type II GeSiSn/Si MQW structures emitting in the range of 1.5–2 μm.
The effect of helium ion irradiation on the microstructure and properties of composites based on Zr/Nb nanoscale multilayer coatings (NMCs) was studied. X-ray diffraction (XRD), transmission electron microscopy (TEM), and variable-energy Doppler broadening spectroscopy (DBS) were used for the in-depth analysis of defects in the irradiated NMCs. After irradiation of the Zr/Nb NMCs with helium ions at a 1017 ion/cm2 dose, the layered structure was generally retained, but the internal stresses in the layers were increased, which caused wave-like distortion in the ion deposition zone. The Zr/Nb NMCs with an individual layer thickness of 25 nm were characterized by the smallest microstress changes, but single blisters were formed in the near-surface region. The microstructure of the Zr/Nb NMCs with a layer thickness of 100 nm exhibited relatively smaller changes upon helium ion irradiation. The prevailing positron-trapping center was the reduced-electron-density area at the interfaces before and after irradiation of the Zr/Nb NMCs regardless of the layer thickness. However, the layer thickness affected the DBS parameter profiles depending on the positron energy, which was probably due to the different localization of implanted ions within the layers or at the interfaces.
Zr/Nb nanoscale multilayer coatings (NMCs) were studied after hydrogenation in a gaseous environment at 400 °C. The hydrogen distribution and content were determined by pressure and hydrogenation time. Increasing the pressure from 0.2 to 2 MPa resulted in different hydrogen distribution within the Zr/Nb NMCs, while the concentration remained constant at 0.0150 ± 0.0015 wt. %. The hydrogen concentration increased from 0.0165 ± 0.001 to 0.0370 ± 0.0015 wt. % when the hydrogenation time was extended from 1 to 7 h. The δ-ZrH hydride phase was formed in the Zr layers with Zr crystals reorienting towards the [100] direction. The Nb(110) diffraction reflex shifted towards smaller angles and the interplanar distance in the niobium layers increased, indicating significant lateral compressive stresses. Despite an increase in pressure, the nanohardness and Young’s modulus of the Zr/Nb NMCs remained stable. Increasing the hydrogen concentration to 0.0370 ± 0.0015 wt. % resulted in a 40% increase in nanohardness. At this concentration, the relative values of the Doppler broadening variable energy positron annihilation spectroscopy (S/S0) increased above the initial level, indicating an increase in excess free volume due to hydrogen-induced defects and changes. However, the predominant positron capture center remained intact. The Zr/Nb NMCs with hydrogen content ranging from 0.0150 ± 0.0015 to 0.0180 ± 0.001 wt. % exhibited a decrease in the free volume probed by positrons, as demonstrated by the Doppler broadening variable energy positron annihilation spectroscopy. This was evidenced by opposite changes in S and W (S↓W↑). The microstructural changes are attributed to defect annihilation during hydrogen accumulation near interfaces with the formation of hydrogen–vacancy clusters and hydrides.