7 February 2020 in Materials
Verified
Journal Article
Open access
PDF file
HCHow-Ji Chen
How-Ji Chen
YYYi-Lin Yu
Yi-Lin Yu
Chao-Wei TangChao-Wei Tang
Chao-Wei Tang
Compared with ordinary concrete, ultra-high performance concrete (UHPC) has excellent toughness and better impact resistance. Under high temperatures, the microstructure and mechanical properties of UHPC may seriously deteriorate. As such, we first explored the properties of UHPC with a designed 28-day compressive strength of 120 MPa or higher in the fresh mix phase, and measured its hardened mechanical properties at seven days. The test variables included: the type of cementing material and the mixing ratio (silica ash, ultra-fine silicon powder), the type of fiber (steel fiber, polypropylene fiber), and the fiber content (volume percentage). In addition to the UHPC of the experimental group, pure concrete was used as the control group in the experiment; no fiber or supplementary cementitious materials (silica ash, ultra-fine silicon powder) were added to enable comparison and discussion and analysis. Then, the UHPC-1 specimens of the experimental group were selected for further compressive, flexural, and splitting strength tests and SEM observations after exposure to different target temperatures in an electric furnace. The test results show that at room temperature, the 56-day compressive strength of the UHPC-1 mix was 155.8 MPa, which is higher than the >150 MPa general compressive strength requirement for ultra-high-performance concrete. The residual compressive strength, flexural strength, and splitting strength of the UHPC-1 specimen after exposure to 300, 400, and 500 °C did not decrease significantly, and even increased due to the drying effect of heating. However, when the temperature was 600 °C, spalling occurred, so the residual mechanical strength rapidly declined. SEM observations confirmed that polypropylene fibers melted at high temperatures, thereby forming other channels that helped to reduce the internal vapor pressure of the UHPC and maintain a certain residual strength.

8 December 2019 in Materials
Verified
Journal Article
Open access
PDF file
HCHow-Ji Chen
How-Ji Chen
CPChing-Fang Peng
Ching-Fang Peng
Chao-Wei TangChao-Wei Tang
Chao-Wei Tang
YCYi-Tien Chen
Yi-Tien Chen
At present, the commonly used repair materials for concrete cracks mainly include epoxy systems and acrylic resins, which are all environmentally unfriendly materials, and the difference in drying shrinkage and thermal expansion often causes delamination or cracking between the original concrete matrix and the repair material. This study aimed to explore the feasibility of using microbial techniques to repair concrete cracks. The bacteria used were environmentally friendly Bacillus pasteurii. In particular, the use of lightweight aggregates as bacterial carriers in concrete can increase the chance of bacterial survival. Once the external environment meets the growth conditions of the bacteria, the vitality of the strain can be restored. Such a system can greatly improve the feasibility and success rate of bacterial mineralization in concrete. The test project included the microscopic testing of concrete crack repair, mainly to understand the crack repair effect of lightweight aggregate concrete with implanted bacterial strains, and an XRD test to confirm that the repair material was produced by the bacteria. The results show that the implanted bacterial strains can undergo Microbiologically Induced Calcium Carbonate Precipitation (MICP) and can effectively fill the cracks caused by external concrete forces by calcium carbonate deposition. According to the results on the crack profile and crack thickness, the calcium carbonate precipitate produced by the action of Bacillus pasteurii is formed by the interface between the aggregate and the cement paste, and it spreads over the entire fracture surface and then accumulates to a certain thickness to form a crack repairing effect. The analysis results of the XRD test also clearly confirm that the white crystal formed in the concrete crack is calcium carbonate. From the above test results, it is indeed feasible to use Bacillus pasteurii in the self-healing of concrete cracks.

9 February 2020 in Sustainability
Verified
Journal Article
Open access
PDF file
HCHow-Ji Chen
How-Ji Chen
MCMING-CHENG CHEN
MING-CHENG CHEN
Chao-Wei TangChao-Wei Tang
Chao-Wei Tang
The interfacial transition zone (ITZ) around aggregates in concrete is a weak area with higher porosity than the matrix; it breaks easily under stress and is not conducive to the durability of concrete. However, the ITZ in concrete is full of calcium hydroxide crystals, which can provide the calcium source required for biomineralization. In view of this, this study aims to use the biological activity (i.e., biomineralization technology) existing in nature to enhance the ITZ in concrete and repair concrete cracks to improve the strength and durability of concrete. In this study, the bacterial strain Sporosarcina pasteurii, which is environmentally friendly, was selected. In addition, lightweight aggregate was used as a bacterial carrier. The bacteria were first sporulated. To protect the strains, the biological species were fixed in porous lightweight aggregates. These lightweight aggregates were then used as concrete aggregates. The planned tests included concrete engineering properties (i.e., compressive strength, chloride ion penetration, and water permeability tests) and residual strength after crack repair. The test results show that the use of lightweight aggregate as a carrier and the implantation of Sporosarcina pasteurii can induce biomineralization, strengthen the ITZ, and repair small internal cracks in concrete, thereby improving the strength and durability of the concrete.

17 May 2021 in Sustainability
Verified
Journal Article
Open access
PDF file
HCHow-Ji Chen
How-Ji Chen
HLHsuan-Chung Lin
Hsuan-Chung Lin
Chao-Wei TangChao-Wei Tang
Chao-Wei Tang
In view of the increasing concerns over non-renewable resource depletion and waste management, this paper studied the development of low-density controlled low-strength material (CLSM) by using stone sludge and lightweight aggregates. First, the investigation was performed at a laboratory scale to assess the effects of the composition on the properties of the resulting low-density CLSM. The Taguchi method with an L9(34) orthogonal array and four controllable three-level factors (i.e., the stone sludge dosage, water to binder ratio, accelerator dosage and lightweight aggregate dosage) was adopted. Then, to optimize the selected parameters, the analysis of variance method was used to explore the effects of the experimental factors on the performance (fresh and hardened properties) of the produced low-density CLSM. The test results show that when the percentage of stone sludge usage was increased from 30% to 60%, the initial setting time approximately doubled on average. Moreover, at the age of 28 days, the compressive strength of most specimens did not exceed the upper limit of 8.83 MPa stipulated by Taiwan’s Public Construction Commission. Further, the material cost per cubic meter of the produced CLSM was about NT$ 720.9 lower than that of the ordinary CLSM, which could reduce the cost by 40.6%. These results indicate that the use of stone sludge as a raw material to produce CLSM could achieve environmental sustainability. In other words, the use of stone sludge and lightweight aggregates to produce low-density CLSM was extremely feasible.

4 November 2022 in Materials
Verified
Journal Article
Open access
PDF file
HCHow-Ji Chen
How-Ji Chen
賢張賢良 張
賢良 張
Chao-Wei TangChao-Wei Tang
Chao-Wei Tang
TYTing-Yi Yang
Ting-Yi Yang
In the field of civil engineering, concrete self-healing technology plays an important role. Concrete self-healing should be able to effectively heal cracks, not only improving the internal structure, but also improving the mechanical properties and durability of the concrete structure. The biomineralization-repair method is characterized by its potential for long-lasting, rapid, and active crack repair potential. Biomineralization repair has an effective bond ability, is compatible with concrete components, and is also environmentally friendly. This study used biomineralization to explore the self-healing of fiber-reinforced lightweight concrete after its exposure to high temperatures. Concrete specimens of a control group (using lightweight aggregate without bacterial spores and a nutrient source) and an experimental group (using lightweight aggregate containing bacterial spores and a nutrient source) were prepared. The repair effect of the microbial self-healing concrete after the exposure to high temperature was observed by a crack-width gauge, field-emission scanning electron microscopy (FESEM), energy-dispersive spectroscopy (EDS), and X-ray diffraction (XRD). According to the EDS and XRD analyses, the precipitate formed at the crack was calcium carbonate. After 28 days of self-healing, the water absorption rate of the experimental group was lower than that of the control group. This is because the specimens of the penetration test were taken from the middle of the concrete cylinder after high temperature, and their bacterial survival rate was higher, which made the mineralization more significant. However, the mechanical test results of the control and experimental groups after the self-healing in the water were not substantially different, which indicated that the bacterial mineralization in the experimental group was slow in the absence of an adequate source of nutrients.

18 September 2021 in Materials
Verified
Journal Article
Open access
PDF file
HCHow-Ji Chen
How-Ji Chen
CCChien-Chuan Chen
Chien-Chuan Chen
HLHung-Shan Lin
Hung-Shan Lin
SLShu-Ken Lin
Shu-Ken Lin
Chao-Wei TangChao-Wei Tang
Chao-Wei Tang
Due to the dense structure of ultra-high-performance concrete (UHPC), it is prone to explosive spalling at high temperatures. In this paper, flexural testing of UHPC and high-strength concrete (HSC) beams was carried out at room temperature and after being subjected to different levels of thermal exposure (300–500 °C). The cross-section of the beam specimen was 150 (width) × 200 (depth) mm, and its length was 1500 mm. The flexural and shear design of the beam specimens were carried out in accordance with the ACI 318M-14 code. All of the beams were singly reinforced with two #4 rebars (minimum reinforcement ratio) as a longitudinal tensile reinforcement at the bottom of the specimen and at an effective depth of 165 mm. The flexural load was applied using the three-point load method. The results show that, at room temperature and after being subjected to different thermal exposures, compared with the HSC specimens, the stiffness of the UHPC specimens in the post-cracking stage was relatively larger and the deflection under a given load was smaller. Moreover, whether at room temperature or after exposure to different thermal exposures, the ductility of the UHPC specimens was better than that of the HSC specimens.