We report high pyroelectricity in lead-free 0.5Ba(Zr0.2Ti0.8)O3–0.5(Ba0.7Ca0.3)TiO3 (BZT–50BCT) ceramics which were previously reported to exhibit high piezoelectricity. The pyroelectric coefficient measured by the Byer–Roundy method upon heating for dc-poled samples shows a high value of 5.84 × 10−4 C m−2 K−1 at 300 K, comparable to those of PZT-based ceramics and significantly higher than many other lead-free pyroelectric materials. The pyroelectric coefficient calculated from the remanent polarization versus temperature relationship obtained during a cooling process is 17.17 × 10−4 C m−2 K−1 at 300 K, which is considerably larger than the value obtained by the Byer–Roundy method. This difference is attributed to the thermal hysteresis of the rhombohedral–tetragonal phase transition between the heating and cooling processes.
Mn-doped (KNN) thin films derived from chemical solution deposition have been investigated. 2 mol % manganese acetate was introduced into the polyvinylpyrrolidone-modified KNN precursor solution to prepare the KNN thin films. It was found that Mn doping can increase the dielectric constant and decrease the dielectric loss, as well as significantly decrease the leakage current. The leakage current density of Mn-doped KNN film is about at an electric field of 50 kV/cm, which is times lower than that of the undoped film (about ). These are attributed to the decrease in the concentration in oxygen vacancies and free carrier-holes by increasing the valence of Mn during thermal treatment. As a result, well saturated polarization-electric field hysteresis loops were obtained in the Mn-doped KNN thin films.
An In2O3/ITO thin film thermocouple was prepared via screen printing. Glass additives were added to improve the sintering process and to increase the density of the In2O3/ITO films. The surface and cross-sectional images indicate that both the grain size and densification of the ITO and In2O3 films increased with the increase in annealing time. The thermoelectric voltage of the In2O3/ITO thermocouple was 53.5 mV at 1270 °C at the hot junction. The average Seebeck coefficient of the thermocouple was calculated as 44.5 μV/°C. The drift rate of the In2O3/ITO thermocouple was 5.44 °C/h at a measuring time of 10 h at 1270 °C.
The un-doped and doped lead-free piezoelectric potassium sodium niobate (K0.5Na0.5NbO3, KNN) ceramics with different amounts of Mn were prepared. The decreased dielectric losses and the improved electrical properties were observed in the Mn-doped KNN ceramics. However, the variation of electrical properties with the Mn contents was not continuously. The 0.5 mol.% Mn-doped KNN ceramic shows the highest dielectric loss and the worst electrical properties. The KNN ceramics doped with less than and more than 0.5 mol.% Mn all show improved electrical properties. The change of lattice position of Mn ions in KNN ceramics was the main reason. When the Mn content is less than 0.5 mol.%, the Mn ions occupied the cation vacancies in A-site. When the Mn content is higher than 0.5 mol.%, the Mn ions entered B-site of KNN perovskite structure and formed the defect complexes ( ) and ( ). They both led to a lower defect concentration. However, When the Mn content is up to 1.5 mol.%, the electrical properties of KNN ceramic became degraded because of the accumulation of Mn oxides at grain boundaries.