Raindrop erosion of wind turbine blades’ leading edge is a critical degradation mechanism limiting wind turbine blade lifetime and aerodynamic efficiency. Protective coatings have been extensively studied to mitigate this damage. This review critically synthesises current knowledge on coating-based protection strategies against erosion, with emphasis on (i) the underlying mechanisms of erosion, (ii) advances in conventional and emerging coating technologies, and (iii) experimental approaches for testing and lifetime prediction. Across reported studies, nanofiller reinforcement (e.g., CNTs, graphene, CeO2, Al2O3) enhances erosion resistance by 60–99%, primarily through improved toughness and stress-wave dissipation. Hybrid and multifunctional systems further combine mechanical durability with self-healing or anti-icing capabilities. Experimental results confirm that erosion rate follows a power-law dependence on impact velocity, with maximum damage occurring between 45° and 60° impact angles. Softer elastomeric coatings demonstrate longer incubation periods and superior viscoelastic recovery compared with rigid sol–gel systems. Persistent gaps include the lack of standardised testing, poor field–lab correlation, and limited long-term durability data. Future work should focus on coordinating multi-stressor testing with variable-frequency rain setups to replicate real field conditions and enable reliable lifetime prediction of next-generation erosion-resistant coatings.
Raindrop erosion of wind turbine blades leading edge is a critical degradation mechanism limiting wind turbine blade lifetime and aerodynamic efficiency. Protective coatings have been extensively studied to mitigate this damage. This review critically synthesises current knowledge on coating-based protection strategies against erosion, with emphasis on (i) the underlying mechanisms of erosion, (ii) advances in conventional and emerging coating technologies, and (iii) experimental approaches for testing and lifetime prediction. Across reported studies, nanofiller reinforcement (e.g., CNTs, graphene, CeO2, Al2O3) enhances erosion resistance by 60 – 99 %, primarily through improved toughness and stress-wave dissipation. Hybrid and multifunctional systems further combine mechanical durability with self-healing or anti-icing capabilities. Experimental results confirm that erosion rate follows a power-law dependence on impact velocity, with maximum damage occurring between 45 ° to 60 ° impact angles. Softer elastomeric coatings demonstrate longer incubation periods and superior viscoelastic recovery compared with rigid sol-gel systems. Persistent gaps include the lack of standardised testing, poor field-lab correlation, and limited long-term durability data. Future work should focus on coordinating multi-stressor testing with variable-frequency rain setups to replicate real field conditions and enable reliable lifetime prediction of next-generation erosion-resistant coatings.
Rain erosion testing of wind turbine blade coatings is still based almost entirely on kinetic test parameters while ignoring the temperature–salinity domains that control field damage. This short communication quantifies how far current rain erosion test conditions diverge from offshore environmental temperature–salinity envelopes. Using seas surface climatology for four offshore regions (North Sea, US Atlantic shelf, Taiwan Strait–South China Sea, Bass Strait) and temperature and water composition parameters from 11 water-based erosion studies, we show the environmental sea surface temperature (SST) spans 5 – 17 °C in the North Sea and 8 – 24 °C in the US Atlantic, rising to 20 – 32 °C in the Asia–Pacific and Bass Strait, with sea surface salinity (SSS) typically 31 – 35.5 PSU. In contrast, all reported droplet erosion tests were run between 18 and 29 °C; three of 11 used only freshwater (~ 0 PSU) and the remainder a single seawater-like level (3.0 – 3.5% NaCl, ≈30 – 35 PSU). No study combined marine salinity with cold (<10 °C) or tropical (≥28 – 30 °C) temperatures, despite evidence of markedly higher damage in saline media and up to an order of magnitude increase in polyurethane rates near the glass transition region.