Pavel Potapov

Pavel Potapov

Auto-generated profile, based on publicly available information

Pavel Potapov


Research Focus & Metrics

Academic Career Length

2Years (2025-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
13 September 2025 in Journal of Composites Science
Verified
Journal Article
Open access
PDF file
Sergey GrigorievSergey Grigoriev
Sergey Grigoriev
MVMarina Volosova
Marina Volosova
VZValery V Zhylinski
Valery V Zhylinski
ESEkaterina Sotova
Ekaterina Sotova
MFMilovich Filipp
Milovich Filipp
Alexey VereschakaAlexey Vereschaka
Alexey Vereschaka
This study investigated the anticorrosive properties of nitride coatings (V,Zr,Nb)N, VN and (Zr,V)N with a thickness of approximately 3 μm, deposited on a substrate of AISI 321 steel. Experiments were conducted in 3.0 and 0.9% aqueous NaCl solutions. The results indicate that the use of (V,Zr,Nb)N, VN and (Zr,V)N coatings to protect AISI 321 steel in corrosive environments (e.g., chloride-containing solutions) allowed corrosion currents to be reduced by 10–20 times (from 7.0 to 0.29 μA/cm2) for a sample with a (Zr,V)N coating in a 3.0% aqueous NaCl solution, and by 2 times (from 0.36 to 0.18 μA/cm2) for a sample with a (V,Zr,Nb)N coating in a 0.9% aqueous NaCl solution. Based on the distribution of elements on the surface of the samples after holding for 168 h in a 3.0% aqueous NaCl solution at 25 °C, it can be qualitatively concluded that the oxidation intensity of the (Zr,V)N coating was the lowest under this condition, and that the VN coating exhibited the highest oxidation intensity among the considered coatings. Analysis of the structure of the (Zr,V)N coating after holding in a 3.0% aqueous NaCl solution for 168 h at 25 °C shows the presence of nanometre-sized chips, while the analysis of the distribution of elements does not record the presence of anything other than the elements comprising the coating. Based on the distribution of elements on the surface of the VN coating, it can be assumed that the destruction of this coating mainly occurs due to peeling off from the substrate; however, corrosion processes also occur in the VN coating itself. Analysis of the distribution of elements in the surface layers of the (V,Zr,Nb)N coating did not show noticeable signs of oxidation. The destruction of this coating occurs due to fragments peeling off from the substrate, while oxidation processes and substrate corrosion do not have a significant effect on the process of (V,Zr,Nb)N coating destruction.

Verified
Journal Article
Open access
PDF file
Sergey GrigorievSergey Grigoriev
Sergey Grigoriev
MVMarina Volosova
Marina Volosova
ESEkaterina Sotova
Ekaterina Sotova
MFMilovich Filipp
Milovich Filipp
Anton SeleznevAnton Seleznev
Anton Seleznev
Alexey VereschakaAlexey Vereschaka
Alexey Vereschaka
To increase wear resistance, (Zr,Nb)N, ZrN and (Zr,Hf)N coatings with columnar structures and (Zr,Ti)N and (Zr,Nb,Hf)N coatings with nanolayer structures were deposited on an AISI 321 stainless steel substrate. The samples with (Zr,Nb)N and ZrN coatings exhibited the best resistance to failure in the scratch test. The sample with the (Zr,Nb)N coating had the best wear resistance for the first 16,000 s. However, eventually the wear of this sample became notable, and after 20,000 s of testing, the lowest degree of wear was observed in the sample with the (Zr,Nb,Hf)N coating. The wear rate of the uncoated sample was 1.5 times greater than that of the sample with the (Zr,Nb,Hf)N coating. The (Zr,Nb,Hf)N coating also exhibited a low degree of indenter mass loss. The (Zr,Nb,Hf)N and ZrN coatings reduced the coefficient of friction (COF) most (COF of approximately 0.20–0.21, compared to COF = 0.28 for the uncoated sample). Defects (nanocavities) were detected in the interface area between the coatings and the substrate, which in some cases can have a negative effect on the wear resistance of the coating. The (Zr,Nb,Hf)N coating (72.07 at.% Zr, 24.87 at.% Nb and 3.05 at.% Hf) had the best wear resistance and a low friction coefficient.

20 September 2026 in Technologies
Verified
Journal Article
Open access
PDF file
Sergey GrigorievSergey Grigoriev
Sergey Grigoriev
PPPavel Potapov
Pavel Potapov
VZValery V Zhylinski
Valery V Zhylinski
UMUladzimir Matys
Uladzimir Matys
ESEkaterina Sotova
Ekaterina Sotova
Alexey VereschakaAlexey Vereschaka
Alexey Vereschaka
This article presents the potential for enhancing the corrosion resistance of stainless steel components by depositing modifying coatings containing copper, chromium, and zirconium layers on their surfaces while optimising the deposition process parameters. Coatings with an outer zirconium nitride (ZrN) or chromium nitride (CrN) layer and adhesive-corrosion-resistant Zr–Cu–Zr, Cr–Cu–Cr, and Cu–Zr sublayers were studied. The highest deposition rate of the copper layer was achieved with a copper cathode arc current of Icat = 85 A and a substrate bias voltage of Usub = 100 V. The proposed coatings reduced corrosion intensity by up to 30 times compared to an uncoated sample and up to three times compared to coatings with an adhesive sublayer without copper (zirconium or chromium only). The use of the proposed coatings reduced corrosion intensity by up to 15 times compared to an uncoated sample and up to 1.6 times compared to coatings with an adhesive layer without copper (chromium only). The Cr–Cu–Cr–CrN coating provided the best corrosion resistance in a 3.0% NaCl solution with a calculated corrosion current icor of 0.36 μA/cm2. These results indicate that the inclusion of a copper layer in the adhesive sublayer provides additional corrosion protection. The sample with a Cr–Cu–Cr–CrN coating exhibited better corrosion resistance, but its adhesive bond to the substrate was not very strong. The sample with a Zr–Cu–Zr–ZrN coating demonstrated high adhesive strength with relatively high corrosion resistance.