Biodegradable or bioresorbable polymers are commonly used in various pharmaceutical fields (e.g., as drug delivery systems, therapeutic systems or macromolecular drug conjugates). Polyesters are an important class of polymers widely utilized in pharmacy due to their biodegradability and biocompatibility features. In recent years, there has been increased interest in enzyme-catalyzed ring-opening polymerization (e-ROP) of cyclic esters as an alternative method of preparation of biodegradable or bioresorbable polymers. Ionic liquids (ILs) have been presented as green solvents in enzymatic ring-opening polymerization. The activity, stability, selectivity of enzymes in ILs and the ability to catalyze polyester synthesis under these conditions are discussed. Overall, the review demonstrates that e-ROP of lactones or lactides could be an effective method for the synthesis of useful biomedical polymers.
In this work, we used the co-precipitation method to synthesize hydroxyapatite (Mn-SeO3-HA) containing both selenium IV (approximately 3.60 wt.%) and manganese II (approximately 0.29 wt.%). Pure hydroxyapatite (HA), hydroxyapatite-containing manganese (II) ions (Mn-HA), and hydroxyapatite-containing selenite ions alone (SeO3-HA), prepared with the same method, were used as reference materials. The structures and physicochemical properties of all the obtained samples were investigated. PXRD studies showed that the obtained materials were homogeneous and consisted of apatite phase. Introducing selenites into the hydroxyapatite crystals considerably affects the size and degree of ordering. Experiments with transmission electron microscopy (TEM) showed that Mn-SeO3-HA crystals are very small, needle-like, and tend to form agglomerates. Fourier transform infrared spectroscopy (FT-IR) and solid-state nuclear magnetic resonance (ssNMR) were used to analyze the structure of the obtained material. Preliminary microbiological tests showed that the material demonstrated antibacterial activity against Staphylococcus aureus, yet such properties were not confirmed regarding Escherichia coli. PACS codes: 61, 76, 81
12 August 2023 in International Journal of Pharmaceutics
Hydroxyapatite (HA) powders enriched with silver or gallium ions or both were synthesized by two different routes: standard precipitation and the solid-state method. The powders were characterized by using several methods: inductively coupled plasma optical emission spectrometry (ICP-OES), powder X-ray diffractometry (PXRD), transmission electron microscopy (TEM), infrared spectroscopy (FT-IR) and solid-state nuclear magnetic resonance spectroscopy (ssNMR). The effects of enrichment of the HAs in Ag+ or Ga3+ or both on in vitro cytotoxicity and microbiological activity were discussed. PXRD experiments showed that the samples obtained by the wet method consisted of single-phase nanocrystalline HA, while the samples prepared via the solid-state method are microcrystalline with a small amount of calcium oxide. The introduction of higher amounts of silver ions was found to be more effective than enriching HA with small amounts of Ag+. Gallium and silver ions were found not to affect the lattice parameters. Ga3+ affected the crystallinity of the samples as well as the content of structural hydroxyl groups. Among samples synthesized by the wet method, only one (5Ag-HAw) was cytotoxic, whereas all Ga-containing samples obtained by the dry method showed cytotoxicity. In the preliminary antimicrobial test all the materials containing “foreign” ions showed high antibacterial activity.