1 February 2017 in Latin American Journal of Solids and Structures
This paper investigates the mechanical properties and corrosion behavior of Metal Matrix Composites prepared using Al7075 alloy as a matrix, Silicon Carbide and Titanium Carbide as reinforcement particles. Two step stir casting process was used to fabricate the composites by varying volume fractions of Silicon Carbide and Titanium Carbide (0 to 15 vol. %). Microstructural analysis, mechanical and corrosion behavior were used to evaluate the performance of the composites. Uniform distribution of reinforcement particle was observed through optical photomicrographs. Vickers micro hardness tests were performed and the hardness values were increased with an increase in reinforcement from 0 to 15 vol. %. The tensile strength of the 10 vol. % of aluminum hybrid matrix composite was better than that of the base alloy. In 3.5% NaCl solution, it was observed that the 15 vol. % of the aluminum hybrid matrix composite have higher corrosion resistance in comparison the base alloy.
16 June 2016 in Proceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture
Metal matrix composites are difficult to machine in traditional machining methods. Abrasive water jet machining is a state-of-the art technology which enables machining of practically all engineering materials. This article deals with the investigation on optimization of process parameters of abrasive water jet machining of hybrid aluminium 7075 metal matrix composites with 5%, 10% and 15% of TiC and B 4 C (equal amount of each) reinforcement. The kerf characteristics such as kerf top width, kerf angle and surface roughness were studied against the abrasive water jet machining process parameters, namely, water jet pressure, jet traverse speed and standoff distance. Contribution of these parameters on responses was determined by analysis of variance. Regression models were obtained for kerf characteristics. Contribution of traverse speed was found to be more than other parameters in affecting top kerf width. Water jet pressure influenced more in affecting kerf angle and surface finish. The microstructures of machined surfaces were also analysed by scanning electron microscopy. The scanning electron microscopy investigations exposed the plastic deformation cutting of hybrid 7075 aluminium metal matrix composite. X-ray diffraction analysis results proved the non-entrapment of abrasive particle on the machined surface.
1 January 2020 in Materials Today: Proceedings
1 January 2020 in Materials Today: Proceedings
18 November 2022 in Journal of Natural Fibers
KDKaruppanasamy Dineshkumar
Karuppanasamy Dineshkumar
Natural fiber reinforced composites are attracting the attention of industries toward a sustainable and environment-friendly material for the future demands. The main drawback pertaining to the use of natural fiber composites lies in its inferior strength in comparison to its counterpart synthetic fibers. This research focuses on improving the fracture toughness of woven jute fabric mat with different orientations (0°, 30° and 45°) in epoxy resin by incorporating fillers and tested in universal tensile testing machine. Silicon carbide (SiC) particles of three sizes 26 µm, 54 µm and 72 µm were incorporated in the matrix in different weight ratios (5%, 10% and 15%). The fracture toughness of the jute/epoxy composites increases with the increase in the amount of SiC particles up to 10% addition and then it shows decreasing trend with further addition. The fracture toughness values show upward trend when the fiber orientation changed from 0° to 45°. Fractography of the tested specimen captured by scanning electron microscope which reveals the fracture of fibers and micro cracks in the epoxy matrix due to the applied load. Analysis of variance (ANOVA) is also conducted for predicting the most influencing parameters on the fracture toughness.
30 March 2021 in Revista de Metalurgia
En el presente trabajo se realiza una investigación sobre las propiedades mecánicas y el comportamiento frente a corrosión del compuesto de matriz metálica Al 7075. El cual se preparó a partir de Al 7075 como matriz y lodo rojo como refuerzo, mediante el uso de un proceso de fundición por agitación en dos pasos. El porcentaje en volumen de refuerzo varía de 0% a 15%. La densidad del material compuesto se calculó mediante el principio de Arquímedes, mayor que la matriz básica. La distribución uniforme del refuerzo y la matriz en el material compuesto se estudió utilizando micrografías ópticas, y la microdureza del material se determinó utilizando una máquina de ensayo de dureza Vickers. La microdureza del compuesto aumentó, mientras que el refuerzo pasó del 0% al 15%. La resistencia a la tracción del material compuesto se elevó al 5% de la tolerancia de refuerzo (326 MPa), que es más alta que la matriz base. Los compuestos de matriz metálica Al 7075 presentan una velocidad de corrosión más baja en una solución de NaCl al 3,5% que la matriz base. A medida que aumenta el porcentaje en volumen en el lodo rojo, se reduce la velocidad de corrosión de los compuestos.