BaTiO3-based piezoelectric ceramics have emerged as highly promising candidates for various applications, due to their excellent piezoelectricity. In this work, the [00l]C textured Ba0.97Ca0.03Ti0.96Sn0.04O3 piezoelectric ceramics were synthesized using the templated grain growth (TGG) method with the assistance of ZnO and Li2O. The effects of ZnO and Li2O on texture development, phase structure, microstructure evolution and electric properties were investigated systematically. Both ZnO and Li2O exhibit a pronounced promoting effect on grain oriented-growth of BCTS, enabling the achievement of an ultra-high texture degree F001 of 98% at a relatively low sintering temperature. More importantly, the incorporation of Li2O in textured BCTS ceramic leads to a substantial enhancement in piezoelectric performance: the piezoelectric coefficient d33, the figure of merit d33 × g33 and maximum strain Sm reach 576 pC/N, 30.6×10⁻¹² m²/N and 0.25%, respectively. The remarkably enhanced piezoelectric response might be attributed to the coeffect of high [001]C grain orientation, multiphase coexistence, refined domain structure and defects engineering. These results clearly demonstrate the great potential of environmentally friendly BCTS-based textured ceramics for applications in piezo-sensors and energy harvesters.
BaTiO3-based ceramics are regarded as one of the promising lead-free alternatives to PZT-based ceramics, and their property enhancement remains one of the most important research directions. This study presents Ba0.96Ca0.04Ti1−xHfxO3-5BT (x = 0.05, 0.07, 0.08, 0.09, 0.10) ceramics with enhanced piezoelectric properties using a crystallographic texture strategy. Highly textured Ba0.96Ca0.04Ti1−xHfxO3-5BT ceramics were successfully prepared by the templated grain growth method, and the effects of Hf content in matrix on the phase structure, morphology, and properties of the textured ceramics were investigated. The textured Ba0.96Ca0.04Ti0.93Hf0.07O3-5BT samples achieved a piezoelectric coefficient d33 of 580 pC/N, an electromechanical coupling factor kt of 0.62, and a high unipolar normalized strain Smax/Emax of 1390 pm/V (measured at 10 kV/cm), together with a strain hysteresis Hs as low as 3.7% under 30 kV/cm, demonstrating excellent piezoelectric properties and favorable strain hysteresis. The excellent comprehensive performance can be attributed to the high-quality preferred orientation and the orthorhombic and tetragonal phase coexistence. Moreover, the multilayer textured Ba0.96Ca0.04Ti0.93Hf0.07O3-5BT ceramics were fabricated by internal electrode co-firing method. The multilayer samples with 10 layers produced a displacement of 581 nm under a driving voltage of 250 V. This study demonstrates that textured BCTH-5BT ceramics can serve as promising eco-friendly lead-free candidates for potential piezoelectric actuation applications.