In this article, a new method has been presented for the estimation of fracture toughness in brittle materials, which enjoys improved accuracy and reduced costs associated with fracture toughness testing procedure compared to similar previous methods, because a vast range of specimens with irregular cracks can be accommodated for testing. Micron-sized alumina powders containing 0.05 wt% magnesium oxide (MgO) nanoparticles were mixed and also together with 2.5 vol%, 5 vol%, 7.5 vol%, 10 vol%, and 15 vol% of silicon carbide (SiC) nanopowders separately. By making and testing various types of ceramics with different mechanical properties, and considering the irregular cracks around the indented area caused by Vickers diamond indenter, a semi-empirical fracture toughness equation has been obtained.
The equation of the Vickers indentation fracture (VIF) proposed by Moradkhani et al. (J. Adv. Ceram. 2, 87–102 (2013)) has been used for the determination of indentation fracture resistance from indented area containing irregular and branch cracks formed around Vickers diamond indentation impressions. The equation is based on the concept that the surface of the micro-cracks is related to the depth of the micro-cracks. Results of the published experimental data have been compared and analyzed with similar and dissimilar methods in all different tested materials, and the accuracy, advantages and disadvantages have been presented and discussed. The results show that, in 90% of the performed tests, the accuracy of the equation is more than 90% compared to methods based on conventional fracture mechanics (CFM) and Vickers indentation fracture (VIF). The results show a high degree of accuracy to date, but the style and method of analysis need to be explained more clearly. Also, there is a requirement for a more comprehensive test range for other brittle materials.
31 May 2019 in Journal of the Korean Ceramic Society
The objective of this research is to analyze the fracture toughness of pure and silica co-doped yttria-stabilized tetragonal zirconia polycrystal (3Y-TZP) bioceramics containing 0.1 and 0.2 wt.% of alumina, and sintered at a temperature of 1500 °C. Because of the relatively easy preparation of the test specimens and the high speed of testing, the Vickers indentation fracture (VIF) technique is more frequently used to evaluate the fracture toughness of biomaterials and hard biological tissues. The Young's modulus and hardness values were obtained by means of nanoindentation and indentation methods. The fracture toughness values of 3Y-TZP bioceramics were calculated and analyzed using 15 equations related to the VIF technique, and loadings of 49.03 and 196.13 N with a Vickers diamond. For validation, the results were compared with fracture toughness values obtained by the single-edge laser-notch beam (SELNB) method with an almost atomically sharp laser-machined initial notch.
28 December 2020 in International Journal of Applied Ceramic Technology