31 January 2011 in Journal of Dental Research
Progress in polymer science has led to continuous reduction of polymerization shrinkage, exemplified by a new generation of “low-shrink composites”. The common inference that shrinkage stress effects will be reduced in teeth restored with such restoratives with lower shrinkage was tested in extracted human premolars. Mesio-occluso-distal slot-shaped cavities were cut and restored with a conventional (SupremePlus) or low-shrink (RefleXions, Premise, Kalore, and LS) composite (N = 5). We digitized the coronal surfaces before and 10 min after restoration to determine cuspal deflection from the buccal and lingual volume change/area. We also determined the main properties involved (total shrinkage, post-gel shrinkage, degree of conversion, and elastic modulus), as well as microleakage, to verify adequate bonding. It was shown that, due to shrinkage stresses, buccal and lingual surfaces pulled inward after restoration (9-14 microns). Only Kalore and LS resulted in significantly lower tooth deformation (ANOVA/Student-Newman-Keuls post hoc, p = 0.05). The other two low-shrink composites, despite having the lowest and highest total shrinkage values, did not cause significant differences in cuspal deflection. Deflection seemed most related to the combination of post-gel shrinkage and elastic modulus. Therefore, even for significantly lower total shrinkage values, shrinkage stress is not necessarily reduced.
1 February 2011 in Dental Materials
24 February 2016 in Journal of Dental Research
The purpose of this study was to investigate the relationship between hygroscopic expansion and polymerization shrinkage for compensation of polymerization shrinkage stresses in a restored tooth. One resin-modified glass-ionomer (RMGI) (Ketac Nano, 3M ESPE), 2 compomers (Dyract, Dentsply; Compoglass, Ivoclar), and a universal resin-based composite (Esthet•X HD, Dentsply) were tested. Volumetric change after polymerization (“total shrinkage”) and during 4 wk of water storage at 37°C was measured using an optical method (n = 10). Post-gel shrinkage was measured during polymerization using a strain gauge method (n = 10). Extracted human molars with large mesio-occluso-distal slot preparations were restored with the tested restorative materials. Tooth surfaces at baseline (preparation), after restoration, and during 4 wk of 37°C water storage were scanned with an optical scanner to determine cuspal flexure (n = 8). Occlusal interface integrity was measured using dye penetration. Data were analyzed using analysis of variance and post hoc tests (significance level 0.05). All tested materials shrunk after polymerization. RMGI had the highest total shrinkage (4.65%) but lowest post-gel shrinkage (0.35%). Shrinkage values dropped significantly during storage in water but had not completely compensated polymerization shrinkage after 4 wk. All restored teeth initially exhibited inward (negative) cuspal flexure due to polymerization shrinkage. Cuspal flexure with the RMGI restoration was significantly less (–6.4 µm) than with the other materials (−12.1 to −14.1 µm). After 1 d, cuspal flexure reversed to +5.0 µm cuspal expansion with the RMGI and increased to +9.3 µm at 4 wk. After 4 wk, hygroscopic expansion compensated cuspal flexure in a compomer (Compoglass) and reduced flexure with Dyract and resin-based composite. Marginal integrity (93.7% intact restoration wall) was best for the Compoglass restorations and lowest (73.1%) for the RMGI restorations. Hygroscopic expansion was more effective in compensating shrinkage stress than would be assumed based on total shrinkage, because only post-gel shrinkage needed compensation. Effective expansion is therefore hygroscopic expansion minus post-gel shrinkage.
1 November 2015 in The Journal of Prosthetic Dentistry
1 September 2015 in Operative Dentistry
SUMMARY: Objectives: To investigate a bulk-fill flowable base composite (Surefil SDR Flow) in terms of cuspal flexure and cure when used in incremental or bulk techniques. Methods: Mesio-occluso-distal cavities (4 mm deep, 4 mm wide) were prepared in 24 extracted molars. The slot-shaped cavities were etched, bonded, and restored in 1) two 2-mm increments Esthet-X HD (control), 2) two 2-mm increments Surefil SDR Flow, or 3) 4-mm bulk Surefil SDR Flow (N=8). The teeth were digitized after preparation (baseline) and restoration and were precisely aligned to calculate cuspal flexure. Restored teeth were placed in fuchsin dye for 16 hours to determine occlusal bond integrity from dye penetration. Extent of cure was assessed by hardness at 0.5-mm increments through the restoration depth. Results were analyzed with analysis of variance and Student-Newman-Keuls post hoc tests (α=0.05). Results: Surefil SDR Flow, either incrementally or bulk filled, demonstrated significantly less cuspal flexure than Esthet-X HD. Dye penetration was less than 3% of cavity wall height and was not statistically different among groups. The hardness of Surefil SDR Flow did not change throughout the depth for both incrementally and bulk filled restorations; the hardness of Esthet-X HD was statistically significantly lower at the bottom of each increment than at the top. Conclusions: Filling in bulk or increments made no significant difference in marginal bond quality or cuspal flexure for the bulk-fill composite. However, the bulk-fill composite caused less cuspal flexure than the incrementally placed conventional composite. The bulk-fill composite cured all the way through (4 mm), whereas the conventional composite had lower cure at the bottom of each increment.
1 July 2015 in The Angle Orthodontist
Objective: : To measure enamel surface changes after ceramic bracket debonding and after cleanup. Materials and Methods: : Forty extracted teeth were scanned in three dimensions using an optical scanner (baseline). Two ceramic bracket systems were placed (19 metal-reinforced polycrystalline ceramic brackets; 21 monocrystalline ceramic brackets). Seven days later, brackets were debonded and teeth scanned (post-debond). Adhesive remnants and bracket fragments were recorded. Tooth surfaces were cleaned using a finishing carbide bur and scanned again (post-cleanup). Post-debond and post-cleanup scans were aligned with the baseline, and surface changes were quantified. Results were statistically compared using t -tests and Mann-Whitney tests (α = .05). Results: : The depth of enamel loss (mean ± standard deviation) post-debond was 21 ± 8 µm and 33 µm and post-cleanup was 28 ± 14 µm and 18 ± 8 µm ( P = .0191); the post-debond remnant thickness was 188 ± 113 µm and 120 ± 37 µm ( P = .2381) and post-cleanup was 16 ± 5 µm and 15 µm for polycrystalline and monocrystalline ceramic brackets, respectively. The monocrystalline ceramic brackets predominantly left all adhesive on the tooth; the polycrystalline ceramic brackets were more likely to leave bracket fragments attached. Conclusion: : Both systems allowed successful removal of the brackets with minimal enamel loss. However, the polycrystalline ceramic brackets left more fragments on the tooth, which complicated cleanup efforts.