21 December 2007 in Journal of Applied Polymer Science
Surface modification of thermotropic liquid crystalline aromatic polyester (LCP) films was examined by low‐pressure plasma treatment to improve initial adhesion and long‐term adhesive reliability between the LCP film and an epoxy bonding sheet for printed circuit boards. Plasma irradiation was carried out in various plasma gases with different plasma modes as reactive‐ion‐etching (RIE), direct‐plasma (DP) with pressures ranging from 4.0 to 26.6 Pa. Although the initial adhesion of the DP‐treated film increased, the long‐term adhesive reliability estimated by pressure cooker test (PCT) decreased with decreasing the plasma gas pressure in every gas. The higher concentration of the generated polar groups such as phenolic hydroxyl group and carboxyl group enhanced the initial adhesion by the increase in the chemical interaction; however, it damaged the long‐term adhesive reliability due to the acceleration of the penetration of water molecules into the interface. The large surface roughness was effective to enhance the initial adhesion and the long‐term adhesive reliability. The RIE‐treatment generated the polar groups and the larger surface roughness than the DP‐treatment. The RIE‐treatment in the O2 atmosphere at the gas pressure of 13.3 Pa was the best plasma condition for both the initial adhesion and the long‐term adhesive reliability. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 2008
22 June 2016 in Journal of Polymer Science Part A: Polymer Chemistry
15 June 2009 in Macromolecules
5 June 2013 in European Polymer Journal
11 March 2005 in Journal of Polymer Science Part A: Polymer Chemistry
1 June 2001 in High Performance Polymers
The control method of poly( p-oxybenzoyl) (POB) whisker length is reported, with the main focus being on how to make the length of the whiskers longer. The POB whiskers were prepared by the polymerization of p-acetoxybenzoic acid in LPF at 330°C. The increase in whisker length is caused by the way oligomer lamellaepileupalongthelongaxisoftheneedle-likecrystalswithspiralgrowth. From the present detailed morphological observations during polymerization, the tip angle of the whiskers is constant at 80° up to a time 10 min, whereas it becomes significantly sharper to 12° at 30 min. This sharpening of the tip angles seems to be highly related to the degree of supersaturation of the oligomers dissolved in solution. In order to depress the sharpening of the tip angle and to extend the steady-state growth for increase of the whisker length, oligomers were added twice into the polymerization system, after 10 min just before the tip angle becomes sharper and then after 20 min. The addition of oligomers extended the steady-state growth period, and the length was increased from 40 μm to 47 μm with the first addition and then to 50 μm with the second addition. The addition of oligomers during steady-state growth gives the most favourable conditions for continuous growth with spiral growth.