The response of titanium surface irradiated with high intensity (1013 – 1015 W/cm2) Ti:sapphire laser was studied in vacuum. Most of the reported investigations were conducted with nano- to femtosecond lasers in gas atmospheres while the studies of titanium surface interacting with femtosecond laser in vacuum are scarce. The laser employed in our experiment was operating at 800 nm wavelength and pulse duration of 60 fs in single pulse regime. The observed surface changes and phenomena are (1) creation of craters, (2) formation of periodic surface structures at the reduced intensity, and (3) occurrence of plasma in front the target. Since microstructuring of titanium is very interesting in many areas (industry, medicine), it can be concluded from this study that the reported laser intensities can effectively be applied for micromachining of the titanium surface (increasing the roughness, formation of parallel periodic surface structures etc.).
14 April 2015 in The International Journal of Advanced Manufacturing Technology
Purpose: This paper aims to report the production of 316L-1 Wt.% NiB cubes by using the selective laser melting (SLM) process. The laser used was pulsed, millisecond Nd:YAG system with maximum average power 100 W. Design/methodology/approach: Densification under different processing conditions (pulse energy, average laser power, laser scan speed, powder layer thickness, pulse frequency) was investigated. Morphology, macro and microstructure of laser melted samples were characterized by digital camera images and by scanning electron microscope. Density of the cubes was determined by Archimedes method in water. Vickers microhardness of samples was determined under the load of 25 g. Corrosion behavior of 316L and 316L-NiB samples was conducted in 5 per cent HCl solution at the testing temperature of 20°C during 240 h. Findings: Using laser power of ∼60-70 W, lower beam overlap and powder layer thickness of 200 µm, 3D cubical samples were obtained with significant balling in individual layers and an overall porosity being around 30 per cent. By increasing laser power to ∼80 W, with higher beam overlap and lower powder layer thickness of 100 µm, SLM parts with no balling and the presence of small pores of up to 4 per cent (20 Hz) and 9 per cent (40 Hz) were obtained. With further increase of laser power to 90 W, overall porosity rose to around 12 per cent. The addition of 1 Wt.% NiB to stainless steel negligibly lowered its corrosion resistance in 5 per cent HCl solution. Originality/value: A part from 316L stainless steel with balling-free structure and good density was successfully obtained through pulsed-SLM process with the aid of 1 Wt.% of NiB addition. Aside from significant influence on the improved structure of cubes, NiB had a favorable effect on microhardness values while practically not affecting the corrosion resistivity of the base material in an aggressive surrounding.
A comparison was made between layer-by-layer laser melting (LM) of two types of feedstock powders: (1) elemental powder blend and (2) mechanically alloyed powder. LM was done by Nd:YAG laser at 1064 nm (max. average power 100 W) in argon ambience. Samples synthesized were Cu-Ti-TiB2 rectangular tracks (20?6?1 mm), and input parameters of the process: powder layer thickness 100-250 ?m, hatch spacing 1 mm, pulse length 4 ms, energy 4 J, pulse repetition rate 20 Hz. Part of the samples was heat-treated in argon at 900 ?C, 10 h. Structural characterization of the samples was done using light microscope and scanning electron microscope (SEM). Chemical analysis of the as-obtained laser melted samples was done by inductively coupled plasma-atomic emission spectrometry (ICP-AES). It was established that the microstructure of LM samples was comprised of Cu-Ti and Cu-B solid regions, and in situ formed microparticles of primary TiB2. Only after high-temperature thermal treatment has the secondary TiB2 occurred. Tensile tests showed much higher strengthening in heat-treated samples with mechanically alloyed powder as starting material, where the formation of secondary TiB2 nanoparticles was considerable.
17 March 2018 in The International Journal of Advanced Manufacturing Technology