28 September 2016 in Journal of Advanced Ceramics
Polymer nanocrystal composites were fabricated by embedding polyvinylidene fluoride (PVDF) with K0.5Na0.5NbO3 (KNN) nanocrystallites of different volume fraction using the hot-pressing technique. For comparison, PVDF–KNN microcrystal composites of the same compositions were also fabricated which facilitated the studies of the crystallite size (wide range) effect on the dielectric and piezoelectric properties. The structural, morphological, dielectric, and piezoelectric properties of these nano and micro crystal composites were investigated. The incorporation of KNN fillers in PVDF at both nanometer and micron scales above 10 vol% resulted in the formation of polar β-form of PVDF. The room temperature dielectric constant as high as 3273 at 100 Hz was obtained for the PVDF comprising 40 vol% KNN nanocrystallites due to dipole–dipole interactions (as the presence of β-PVDF is prominent), whereas it was only 236 for the PVDF containing the same amount (40 vol%) of micron-sized crystallites of KNN at the same frequency. Various theoretical models were employed to predict the dielectric constants of the PVDF–KNN nano and micro crystal composites. The PVDF comprising 70 vol% micron-sized crystallites of KNN exhibited a d33 value of 35 pC/N, while the nanocrystal composites of PVDF–KNN did not exhibit any piezoelectric response perhaps due to the unrelieved internal stress within each grain, besides the fact that they have less domain walls.
18 May 2007 in Journal of Materials Science
27 March 2002 in Journal of Materials Chemistry
Glass nanocomposites in the system (100 − x)Li2B4O7–xSrBi2Ta2O9 (0 ≤ x ≤ 22.5, in molar ratio) were fabricated via a melt quenching technique followed by controlled heat-treatment. The as-quenched samples were confirmed to be glassy and amorphous by differential thermal analysis (DTA) and X-ray powder diffraction (XRD) techniques, respectively. The phase formation and crystallite size of the heat-treated samples (glass nanocomposites) were monitored by XRD and transmission electron microscopy (TEM). The relative permittivities (εr′) of the glass nanocomposites for different compositions were found to lie in between that of the parent host glass (Li2B4O7) and strontium bismuth tantalate (SBT) ceramic in the frequency range 100 Hz–40 MHz at 300 K, whereas the dielectric loss (D) of the glass nanocomposite was less than that of both the parent phases. Among the various dielectric models employed to predict the effective relative permittivity of the glass nanocomposite, the one obtained using the Maxwell’s model was in good agreement with the experimentally observed value. Impedance analysis was employed to rationalize the electrical behavior of the glasses and glass nanocomposites. The pyroelectric response of the glasses and glass nanocomposites was monitored as a function of temperature and the pyroelectric coefficient for glass and glass nanocomposite (x = 20) at 300 K were 27 µC m−2 K−1 and 53 µC m−2 K−1, respectively. The ferroelectric behavior of these glass nanocomposites was established by P vs. E hysteresis loop studies. The remnant polarization (Pr) of the glass nanocomposite increases with increase in SBT content. The coercive field (Ec) and Pr for the glass nanocomposite (x = 20) were 727 V cm−1 and 0.527 µC cm−2, respectively. The optical transmission properties of these glass nanocomposites were found to be composition dependent. The refractive index (n = 1.722), optical polarizability (αm = 1.266 × 1023 cm3) and third-order nonlinear optical susceptibility (χ(3) = 3.046 × 10−21 cm3) of the glass nanocomposite (x = 15) were larger than those of the as-quenched glass. Second harmonic generation (SHG) was observed in transparent glass nanocomposites and the deff for the glass nanocomposite (x = 20) was found to be 0.373 pm V−1.
30 September 2006 in Optical Materials
BVB. Harihara Venkataraman
16 February 2005 in Journal of the American Ceramic Society