The cobalt white alloy, an intermediate product of cobalt smelting, is difficult to leach at atmosphere due to its corrosion-resistant structure. The current study proposed a novel process to extract Co and Cu from the cobalt white alloy with high silicon content. The process mainly involves three steps: desilication of the alloy melt through oxidation smelting using MnO-MgO-SiO2 slag, powder making of the desilication alloy melt by water atomization and atmospheric sulfuric acid leaching of the alloy powders. The results showed that 83.64% of Si in the white alloy was removed effectively by oxidizing it preferentially into the MnO-MgO-SiO2 slag. 97.99% of cobalt and 97.78% of copper were leached under optimal conditions according to: temperature of 95 °C, liquid/solid ratio of 10/1, excess of sulfuric acid of 1.3 times the stoichiometric demand, stirring rate of 1500 rpm, leaching time of 8.0 hours, and oxygen gas flow rate of 0.15 L/min. The overall recovery in this process attained 93.41% for cobalt and 94.33% for copper, separately.
15 January 2022 in International Journal of Minerals, Metallurgy and Materials
As a fundamental study related to spent lithium-ion batteries recycling by a combined pyro- and hydro- metallurgical process, the solubility of nickel in alumina saturated MnO-SiO2-Al2O3 slags in equilibrium with Cu-Ni alloy has been investigated under controlled oxygen potentials of 5.5 × 10−11 atm, 5.5 × 10−12 atm, and 5.5 × 10−13 atm at 1573 K. The results show that nickel dissolved in the slags mainly exists as NiO. The nickel solubility in the slags increased with the increase of nickel concentration in the alloy, and increased with increasing oxygen potential at a given concentration of nickel in the alloy. The activity coefficient of NiO in the slag relative to the pure solid standard, γNiO(s), increased with increasing NiO content in the slag, and can be calculated by the following equation: γNiO(s) = 46.77(wt.% NiO in slag) + 9.85, where (wt.% NiO) represents mass percent of NiO in the slag.