For first time, new innovative ruthenium N3-Dye anchored with selenium (Se) and N3 dye anchored with sulphur atoms were synthesized in a good yield. Dyes are applied and evaluated in performance of dye sensitized solar cell. N3–Se dye showed superior photochemical& electrochemical behavior and high rate electron transfer across anode surface than N3–S dye. The better optical and electrochemical activities would make Se-dye a candidate for applications in solar cells. Half life time of N3–S showed a single exponential decay with an average lifetime of 0.8 ns. For N3–Se dye, decay curve was fitted by sum two exponential functions with 75% and 25% counts have 2.5 ns and 30 ns respectively. Solar cells were fabricated and analyzed to determine their solar-to-electric conversion efficiency under standard AM 1.5 sunlight. Commercial N3 dyes showed current density (Jsc) of 17.813 mA cm−2, open circuit potential (Voc) of 0.678 V, filling factor (FF) of 0.607 and conversion efficiencies (η) of 7.3%. Corresponding values for N3–S dye, Jsc 11.2 mA cm−2, Voc 0.650 V, FF 0.681 and η 5%. Se–N3 dye, showed Jsc = 6.670 mA cm−2, Voc = 0.6004 V, FF = 0.77 and η = 3.09%. Long lifetime of N3–Se caused low practical performance.
Nanocrystalline TiO2 and reduced graphene oxide (rGO) materials have been synthesized by a simple and low-cost microwave-assisted hydrothermal method and applied in dye-sensitized solar cells (DSSCs) as photoactive and metal-free counter electrodes, respectively. Different TiO2 nanocrystalline materials have been synthesized via the acid hydrolysis sol-gel method, followed by microwave hydrothermal treatment at 210 °C and 300 psi and at different microwave irradiation times (20, 30, 45, and 60 min) instead of the usual hydrothermal time of 12 h. The properties of the produced mesoporous nanocrystalline TiO2 are investigated in terms of their morphology, crystal structure, optical properties, and surface area behavior using relevant characterization techniques. Maximum specific surface area values (SBET) of 97.77 and 100.7 m2 g-1 are measured for TiO2, with the average crystallite sizes of 18.6 and 17.5 nm, at microwave irradiation times of 30 and 45 min, respectively. Different rGO samples have been prepared by the modified Hummers method, followed by microwave-assisted reduction at a temperature of 200 °C and pressure of 300 psi at different microwave irradiation times (3, 17, and 25 min). The physicochemical properties of the different rGO samples in terms of morphology, crystallization, and optical properties are characterized by TEM, XRD, and Raman spectroscopic analysis. The current density Jsc of the fabricated DSSCs based on TiO2 as the photoelectrode and rGO as the counter electrode compared with DSSCs based on Pt as the counter electrode is found to be 11.25 and 9.28 mA cm-2, respectively. Although the overall power efficiency of the fabricated DSSCs based on rGO as the counter electrode is lower than that based on the Pt electrode, the former still exhibits promising prospects for replacing Pt with low-cost metal-free carbon-based DSSCs.
29 March 2023 in Journal of Materials Science: Materials in Electronics
In this article, InP quantum dots (QDs) are synthesized with a green methodology. The preparation of the InP QDs is demonstrated by varying the ratios of the precursors used such as InCl3 and trioctylphosphine (TOP). These QDs are fabricated through the application of TOP (as phosphorous source and reducing agent for the In salt) for forming indium and to develop the targeted InP QDs, which are characterized using HRTEM, XRD, PL, FTIR, UV–Vis, and time resolved spectroscopy. A rapid reaction time (~ 30 min) procedure in a single pot at a temperature of ~ 310 °C is developed. InP QDs with particle sizes varying from 4 to 6 nm have been measured with different concentrations of InCl3 and TOP. InP QDs yield reached 23%. Zincblende crystal structure is recognized for InP with high orientation plane of (220) as confirmed with XRD and confirmed with SAED. Solar cell devices are built by anchoring the InP QDs onto a TiO2 layer and measure the photovoltaic performance and spectral response of the device built on FTO/glass substrate. TiO2/InP QDs solar cell devices are fabricated with high fill factor of 0.86 and open circuit voltage value of 501 mV and overall efficiency of 0.48%.
In this study, we investigated an innovative method for the fabrication of nanostructure bulk alloys and thin films of indium gallium nitride (InxGa1−xN) as active, thin films for light-emitting diode (LED) devices using both crystal growth and thermal vacuum evaporation techniques, respectively. These methods resulted in some tangible improvements upon the usual techniques of InxGa1−xN systems. A cheap glass substrate was used for the fabrication of the LED devices instead of sapphire. Indium (In) and Gallium (Ga) metals, and ammonia (NH3) were the precursors for the alloy formation. The alloys were prepared at different growth temperatures with compositions ranging from 0.1 ≤ x ≤ 0.9. InxGa1−xN alloys at 0.1 ≤ x ≤ 0.9 had different crystallinities with respect to X-Ray diffraction (XRD) patterns where the energy bandgap that was measured by photoluminescence (PL) fell in the range between 1.3 and 2.5 eV. The bulk alloys were utilized to deposit the thin films onto the glass substrate using thermal vacuum evaporation (TVE). The XRD thin films that were prepared by TVE showed high crystallinity of cubic and hexagonal structures with high homogeneity. Using TVE, the InxGa1−xN phase separation of 0.1 ≤ x ≤ 0.9 was eliminated and highly detected by XRD and FESEM. Also, the Raman spectroscopy confirmed the structure that was detected by XRD. The FESEM showed a variance in the grain size of both alloys and thin films. The InxGa1−xN LED device with the structure of glass/GaN/n-In0.1Ga0.9N:n/In0.1Ga0.9N/p-In0.1Ga0.9N:Mg was checked by the light emitted by electroluminescence (EL). White light generation is a promising new direction for the fabrication of such devices based on InxGa1−xN LED devices with simple and low-cost techniques.
In this study, we investigate a novel simple methodology to synthesize gallium nitride nanoparticles (GaN) that could be used as an active layer in light-emitting diode (LED) devices by combining the crystal growth technique with thermal vacuum evaporation. The characterizations of structural and optical properties are carried out with different techniques to investigate the main featured properties of GaN bulk alloys and their thin films. Field emission scanning electron microscopy (FESEM) delivered images in bulk structures that show micro rods with an average diameter of 0.98 µm, while their thin films show regular microspheres with diameter ranging from 0.13 µm to 0.22 µm. X-ray diffraction (XRD) of the bulk crystals reveals a combination of 20% hexagonal and 80% cubic structure, and in thin films, it shows the orientation of the hexagonal phase. For HRTEM, these microspheres are composed of nanoparticles of GaN with diameter of 8–10 nm. For the optical behavior, a band gap of about from 2.33 to 3.1 eV is observed in both cases as alloy and thin film, respectively. This article highlights the fabrication of the major cubic structure of GaN bulk alloy with its thin films of high electron lifetime.
In0.1Ga0.9N thin film was grown on a cheap glass substrate by the Nd:YAG pulsed laser deposition technique. The In0.1Ga0.9N thin films show the semi-crystalline structure as observed with X-ray diffraction (XRD). The surface morphology has a non-dense layer with both scattered nanospheres and agglomerated particles. These nanospheres tended to grow randomly on the glass substrate, as observed with field emission scanning electron microscopy (FESEM). The direct bandgap energy for In0.1Ga0.9N thin film was 2.08 eV, which is calculated using photoluminescence (PL) measurements. The Raman measurements illustrated two sets of phonon modes as A1(LO) and E2 high vibrational modes that are observed. The resonance behavior of the A1(LO) mode is experimentally verified and studied under laser light energy of 532 nm.