1 January 2009 in Dental Materials Journal
Verified
Journal Article
Open access
PDF file
SOSeigo Okawa
Seigo Okawa
KWKouichi Watanabe
Kouichi Watanabe
Chemical mechanical polishing (CMP) of cpTi (Ti) was carried out using two types of slurries, acidic and basic colloidal silica containing H2O2 up to 3 wt%, to obtain flat and mirror-polished surfaces without any contaminated and reacted layers. Polishing behavior and surface properties were investigated using AFM, EPMA, and XPS. Weight loss of Ti polished by CMP using the basic slurry was larger than that using the acidic one, and surface roughness was less than 2 nm RMS when basic slurry containing 3 wt% H2O2 was used. Moreover, three kinds of chemical species, OH-, O2-, and H2O, were detected on the Ti surfaces polished by CMP using these slurries. Results of this study showed that CMP using colloidal silica containing H2O2 successfully created a mirror-polished surface without contaminated and reacted layers.

Verified
Journal Article
Open access
PDF file
SOSeigo Okawa
Seigo Okawa
NTNorimasa Taka
Norimasa Taka
YAYujin Aoyagi
Yujin Aoyagi
We investigated the effect of helium atmospheric-pressure plasma (PL) and deep-ultraviolet (UV) light treatments on the adhesive properties of fiber-reinforced poly(ether-ether-ketone) polymer (PEEK). PEEK disks reinforced with carbon (CPEEK) or glass (GPEEK) fibers were polished, modified with PL and UV for 60 s, and the surface energy was calculated by measuring the contact angles. The disk surfaces were analyzed by X-ray photoemission spectroscopy. Shear bond strength testing was performed using a universal testing machine, and the fracture surfaces were observed by electron probe microanalyzer. Data were analyzed with one and two-way ANOVA and Tukey’s post-hoc test (p < 0.05). The surface energies were increased by the modifications, which created OH functional groups on the surfaces. The bond strengths of CPEEK were increased by PL, and those of GPEEK were increased by PL and UV, owing to chemical bonding at the interface.

1 January 2004 in Dental Materials Journal
Verified
Journal Article
Closed access
PDF file
SOSeigo Okawa
Seigo Okawa
AHAwlad Hossain
Awlad Hossain
MKMitsugu Kanatani
Mitsugu Kanatani
KWKouichi Watanabe
Kouichi Watanabe
OMOsamu Miyakawa
Osamu Miyakawa
Electrochemical buffing, a combined process of electrochemical and mechanical polishing, was applied to titanium casting. Mixture of α-Al2O3 suspension (average grain diameter of 5μm) and 5% KNO3 solution was used as abrasive slurry. Specimen and experimental wheel buff were respectively connected to the positive and negative poles of a DC source, whose potential ratings ranged from 0V (MEP) to 10V (ECB10). Surface roughness, hardness, color, and cleanness were investigated. ECB10 surface produced a gold color and attained a mirror finish, as its roughness value was only one-quarter that of MEP. High amount of aluminum was present in MEP surface. Its bond state entirely differed from that of α-Al2O3, hence indicating surface alteration due to chemical reactions with the abrasive material. At higher potentials, reaction products might be dissolved anodically, so that the surface was chemically clean to some extent. The surface also became rich in OH-.

1 January 2009 in Dental Materials Journal
Verified
Journal Article
Closed access
PDF file
SOSeigo Okawa
Seigo Okawa
KHKikuo Homma
Kikuo Homma
MKMitsugu Kanatani
Mitsugu Kanatani
KWKouichi Watanabe
Kouichi Watanabe
Electrochemical deposition of calcium phosphate (CAP) on valve metals such as Ta, Nb, and Zr, was performed by anodic oxidation with alternate polarity inversion at an applied 20 VDC. A saturated hydroxyapatite(HAP)-phosphoric acid solution (pH 3) was used as the electrolyte. FTIR, XRD, and XPS were employed to investigate the detailed characteristics of the deposition. HAP was precipitated on Ta; HAP including brushite and monetite on Nb; and HAP and monetite on Zr. The Ca/P atomic ratios were 1.3-1.5 by XPS, and HPO42– bands were detected on Ta by FTIR. Therefore, the HAP precipitated on Ta was a Ca-deficient HAP. In addition, the XPS spectra of the specimens showed that phosphate ions were incorporated into the anodic oxide film. Deposits with nano-grain size were observed by AFM. The results confirmed that CAP with nano-grain size was deposited on valve metals by the anodic oxidation with polarity inversion.

1 January 1982 in Dental Materials Journal
Verified
Journal Article
Closed access
KWKouichi Watanabe
Kouichi Watanabe
SOSeigo Okawa
Seigo Okawa
OMOsamu Miyakawa
Osamu Miyakawa
SNSyuji Nakano
Syuji Nakano
NSNobuhiro Shiokawa
Nobuhiro Shiokawa

1 January 1996 in Dental Materials Journal
Verified
Journal Article
Closed access
KWKouichi Watanabe
Kouichi Watanabe
SOSeigo Okawa
Seigo Okawa
MKMitsugu Kanatani
Mitsugu Kanatani
SNSyuji Nakano
Syuji Nakano
OMOsamu Miyakawa
Osamu Miyakawa
MKMasayoshi Kobayashi
Masayoshi Kobayashi
The possibility of the segregation under solidification process using a centrifugal casting machine was investigated using an electron probe microanalyzer with elemental distribution map, line analysis and quantitative analysis. When a very small quantity of platinum was added to local molten titanium during the casting process, macroscopic segregation was observed under conditions of density difference of 0.1 g/cm3 at the most, confirming that the centrifugal force of the casting machine is extremely strong. When a Ti-6Al-4V alloy was cast, however, no macroscopic segregation was observed. The centrifugal force of the casting machine examined in the present study hardly results in the body-force segregation in this titanium alloy.