The relationship among the Wigner crystal, charge ordering, and the Mott insulator is studied by the path-integral renormalization group method in two-dimensional systems with long-range Coulomb interaction. In contrast to the insensitivity of the Hartree-Fock results, the stability of the solid drastically decreases with the decrease in the lattice commensurability. The transition to liquid occurs at the electron gas parameter for the filling , showing a large reduction from in the continuum limit. A correct account of quantum fluctuations is crucial to understanding the charge-order stability generally observed only at simple fractional fillings and the nature of quantum liquids away from them.
8 November 2016 in Journal of Applied Crystallography
Dynamic nuclear polarization (DNP) at low temperature (1.2 K) and high magnetic field (3.3 T) was applied to a contrast variation study in small-angle neutron scattering (SANS) focusing on industrial rubber materials. By varying the scattering contrast by DNP, time-of-flight SANS profiles were obtained at the pulsed neutron source of the Japan Proton Accelerator Research Complex (J-PARC). The concentration of a small organic molecule, (2,2,6,6-tetramethylpiperidine-1-yl)oxy (TEMPO), was carefully controlled by a doping method using vapour sorption into the rubber specimens. With the assistance of microwave irradiation (94 GHz), almost full polarization of the paramagnetic electronic spin of TEMPO was transferred to the spin state of hydrogen (protons) in the rubber materials to obtain a high proton spin polarization (PH). The following samples were prepared: (i) a binary mixture of styrene–butadiene random copolymer (SBR) with silica particles (SBR/SP); and (ii) a ternary mixture of SBR with silica and carbon black particles (SBR/SP/CP). For the binary mixture (SBR/SP), the intensity of SANS significantly increased or decreased while keeping its q dependence for PH = −35% or PH = 40%, respectively. The q behaviour of SANS for the SBR/SP mixture can be reproduced using the form factor of a spherical particle. The intensity at low q (∼0.01 Å−1) varied as a quadratic function of PH and indicated a minimum value at PH = 30%, which can be explained by the scattering contrast between SP and SBR. The scattering intensity at high q (∼0.3 Å−1) decreased with increasing PH, which is attributed to the incoherent scattering from hydrogen. For the ternary mixture (SBR/SP/CP), the q behaviour of SANS was varied by changing PH. At PH = −35%, the scattering maxima originating from the form factor of SP prevailed, whereas at PH = 29% and PH = 38%, the scattering maxima disappeared. After decomposition of the total SANS according to inverse matrix calculations, the partial scattering functions were obtained. The partial scattering function obtained for SP was well reproduced by a spherical form factor and matched the SANS profile for the SBR/SP mixture. The partial scattering function for CP exhibited surface fractal behaviour according to q−3.6, which is consistent with the results for the SBR/CP mixture.
A method of time-of-flight, small-angle neutron scattering (TOF-SANS) has been developed based on the iMATERIA powder diffractometer at BL20, of the Materials and Life Sciences Facility (MLF) at the high-intensity proton accelerator (J-PARC). A large-area detector for SANS, which is composed of triple-layered 3He tube detectors, has a hole at its center in order to release a direct beam behind and to detect ultra-small-angle scattering. As a result, the pulsed-neutron TOF method enables us to perform multiscale observations covering 0.003 < q (Å−1) < 40 (qmax/qmix = 1.3 × 104) and to determine the static structure factor S(q) and/or form factor P(q) under real-time and in-situ conditions. Our challenge, using unique sample accessories of a super-conducting magnet and polarized neutron, is dynamic nuclear polarization (DNP) for contrast variation, especially for industrial use. To reinforce conventional SANS measurements with powder materials, grazing-incidence small-angle neutron scattering (GISANS) or reflectivity is also available on the iMATERIA instrument.
It is proposed that nanosized graphene aggregation could facilitate coherent neutron scattering under particle size conditions similar to nanodiamonds to enhance neutron intensity below cold neutrons. Using the RIKEN accelerator-driven compact neutron source and iMATERIA at J-PARC, we performed neutron measurement experiments, total neutron cross-section and small-angle neutron scattering on nanosized graphene aggregation. For the first time, the measured data revealed that nanosized graphene aggregation increased the total neutron cross-sections and small-angle scattering in the cold neutron energy region. This is most likely due to coherent scattering, resulting in higher neutron intensities, similar to nanodiamonds.
Recently, we have developed a novel dynamic nuclear polarization (DNP) apparatus with a magnetic field of 7 T and a sample temperature of 1 K. High proton spin polarizations from −84% to 76%, for TEMPO doped polystyrene samples, have been demonstrated. This DNP apparatus satisfies the simultaneous requirement for quick and easy sample exchange and high DNP performance. On the iMATERIA (BL20) instrument at J-PARC, the first beam experiment using this DNP apparatus has been performed. For this experiment, the beamline was equipped with a supermirror polarizer. The stray magnetic field due to the superconducting magnet for DNP was also evaluated. The stray magnetic field plays an important role for in maintaining the neutron polarization during the transportation from the polarizer to the sample. The small-angle neutron scattering (SANS) profiles of silica-filled rubber under dynamically polarized conditions are presented. By applying our new analytical approach for SANS coherent scattering intensity, neutron polarization (PN) as a function of neutron wavelength was determined. Consequently, for the neutron wavelength, range from 4 Å to 10 Å, |PN| was sufficient for DNP-SANS studies.