Fluorine/silicone composite rubber is widely used as a sealing material in aerospace, missile, automotive, petroleum, and other industries, but the traditional process does not use synergistic fillers to strengthen the composite system. In this research, fumed SiO2 and black caron (N990) were used as synergistic fillers, fluorine/silicone composite rubber was prepared by mechanical mixing process, and three different fluorine rubber systems were used to find the best composite material. The mechanical properties, thermal properties, aging properties, moderate strength properties, and microstructure of the composites were evaluated. Studies have shown that mixing the two can produce a certain interface interaction and effectively improve the compatibility. The physical properties of the material tended to decrease during the increase in the added amount of silicone rubber (MVQ). The maximum tensile strength of the hybrid material can reach 15 MPa. The optimal mixing ratio is fluororubber/silicone rubber (FKM/MVQ) = 9/1. At this time, the mechanical properties of the composite material are in the best state, and SiO2 and black caron (N990) have a reinforcing effect, which can effectively improve the mechanical properties. After the composite was kept at 200 °C for 48 h, the tensile strength and elongation of the best sample A1 were 99.5 and 97.0%, respectively, showing excellent anti-aging properties. This work provides a method to fabricate high-strength fluorine/silicone composites using synergistic fillers that may be used in heat-medium-sealed environments.
Tin dioxide (SnO 2 ) photocatalyst has broad prospects for the degradation of toxic organic pollutants; however, its practical application is greatly hampered by poor activity due to the high recombination rates of photogenerated electron‐hole pairs. In this work, titania (TiO 2 ) modified SnO 2 photocatalysts were obtained by a facile hydrothermal method to suppress the rapid recombination of photogenerated electron‐hole pairs and improve the photocatalytic activity. Ultraviolet–visible (UV–vis)_ diffuse reflectance spectra suggest that TiO 2 –SnO 2 composite photocatalysts hold stronger UV light absorption ability than that of the pure SnO 2 . Surface photovoltage spectroscopy and photoelectrochemistry results show that the separation rate of photogenerated charge pairs of TiO 2 –SnO 2 photocatalysts was greatly enhanced. The photocatalytic activities of the photocatalysts were evaluated by the decay of rhodamine B (RhB) under UV irradiation illumination. The results display that modification of SnO 2 by TiO 2 can largely enhance the photocatalytic activity and the photocatalytic performance of 0.5:1‐TS sample is nearly 5 times that of the pure SnO 2 . Moreover, maintaining the ratio of TiO 2 and SnO 2 at 0.5:1, the amount of catalyst was 30 mg, the concentration of dye was 10 mg/l, and the pH of RhB solution was 2, the sample has the best photocatalytic activity.
Polyvinylidene fluoride (PVDF) binder is an important part of lithium-ion batteries, where a slight structural difference can significantly affect the capacitance and service life of batteries. Herein, ATR-FTIR technology and a rheological test were employed to investigate the crystal forms and rheological behavior of three different PVDF binders, respectively. The results showed that PVDF-CG has low molecular weight, high α/β phase ratio, strong adhesive action and stripping strength, which are closely associated with the durability and electrochemical properties of LiNi0.5Co0.2Mn0.3O2 single-crystal (denoted as SC) materials. The SCs with PVDF-CG binder exhibited a capacity retention of 93.44% after 100 cycles at a rate of 1C and high rate performance (92 mA h g−1 at 10C), which was higher than that of PVDF-HSV900 (90.31%, 86 mA h g−1 at 10C) and PVDF-Solvay 5130 (90.52%, 72 mA h g−1 at 10C). The XPS and HR-TEM analysis showed that the cycled SCs bonded with HSV900 and Solvay 5130 as binders suffered from severe interface structural degradation, while SCs with PVDF-CG maintained a well-layered structure and the formation of a surface NiO-like rock-salt phase was greatly inhibited. This work demonstrated that the capacity, rate capability and interface stability of SC cathodes are significantly affected by the mode and strength of the adhesion and stripping strength of PVDF binders, which are closely associated with α/β phase ratios, providing a useful reference for the development of efficient binders.
15 October 2024 in Journal of Materials Chemistry A
Fluoride-ion batteries (FIBs) offer a high theoretical energy density of 5000 W h L−1 and superior safety, but they face significant challenges such as electrode material dissolution and volume changes during cycling. Herein, this study presents an advanced interface engineering strategy to enhance the stability of the electrolyte–electrode interface. Through plasma treatment, substrate surface energy and adhesion are increased, while a co-deposition device generates a high-energy ion beam (Bi3+ and F−), depositing atoms densely and uniformly on CuF2 to form a protective layer. Additionally, regulating the BiOxFy crystal structure via controlled O2− ion injection optimizes F− transport and diffusion barriers. This modulation, driven by O-2p and F-2p electron density states, retards F− diffusion kinetics and mitigates volume changes in CuF2 during cycling. The resulting battery showed stable performance in N,N,N-dimethyl-N,N-dineopentylammonium fluoride liquid electrolyte at room temperature, including a specific capacity of 110 mA h g−1 and a fiftyfold longer cycling life than that of existing Cu@LaF3 core–shell batteries. Furthermore, X-ray absorption fine structure analysis reveals the pivotal role of a BiOF film in mitigating the lattice recombination effect by assimilating excess F−. These findings highlight the importance of this advanced interface strategy for advancements in FIBs.