This paper presents the analysis of the friction stir-processed aluminium alloy 5083-H111 gas tungsten arc-welded and friction stir-welded joints. The comparative analysis was performed on the processed and unprocessed gas tungsten arc-welded and friction stir-welded joints of similar aluminium alloy 5083-H111. The results showed a clear distinction between the friction stir processed joints and unprocessed joints. There is a good correlation observed between the microstructural results and the tensile results. Ultrafine grain sizes of 4.62 μm and 7.177 μm were observed on the microstructure of the friction stir-processed friction stir-welded and gas tungsten arc-welded joints. The ultimate tensile strength for friction stir-welded and gas tungsten arc-welded before friction stir processing was 153.75 and 262.083 MPa, respectively. The ultimate tensile strength for friction stir processed friction stir-welded joint was 303.153 MPa and gas tungsten arc-welded joints one was 249.917 MPa. The microhardness values for the unprocessed friction stir-welded and gas tungsten arc-welded joints were both approximately 87 HV, while those of the friction stir-processed ones were 86.5 and 86 HV, respectively. The application of friction stir processing transformed the gas tungsten arc morphology from brittle to ductile dimples and reduced the ductile dimple size of the unprocessed friction stir-welded joints from the range of 4.90–38.33 μm to 3.35–15.59 μm.
There is an increase in reducing the weight of structures through the use of aluminium alloys in different industries like aerospace, automotive, etc. This growing interest will lead towards using dissimilar aluminium alloys which will require welding. Currently, tungsten inert gas welding and friction stir welding are the well-known techniques suitable for joining dissimilar aluminium alloys. The welding of dissimilar alloys has its own dynamics which impact on the quality of the weld. This then suggests that there should be a process which can be used to improve the welds of dissimilar alloys post their production. Friction stir processing is viewed as one of the techniques that could be used to improve the mechanical properties of a material. This paper reports on the status and the advancement of friction stir welding, tungsten inert gas welding and the friction stir processing technique. It further looks at the variation use of friction stir processing on tungsten inert gas and friction stir welded joints with the purpose of identifying the knowledge gap.
The submerged friction stir processing (SFSP) technique was employed on the prior friction stir welded (FSW) AA6082/AA8011 dissimilar aluminum alloy joints. The tap water with room temperature was kept at 40 mm depth throughout the processing. The AA6082 was kept at the advancing side during FSW and SFSP process and this was done to enhance the strength of the joint. The SFSP joints were studied comparatively with the FSW joints. The sampling position was also studied for both the FSW joint and SFSP joint. The employment of the submerged friction stir processing resulted in the microstructural grain size refinement. The tensile strength of the SFSP joint was found to be higher than that of AA8011 base metal but lower than that of AA6082 base metal. The tensile strength of the FSW joint was found to be lower than that of both base metals. There was a clear correlation between the tensile properties and the grain size refinement. The SFSP joint exhibited good microhardness properties compared to the FSW joint.
The problems associated with the fabrication of in situ metal matrix composites (MMC) by conventional methods can be avoided by using microwave sintering and friction stirring in combination. The current study investigates the mechanical and electrical properties of pure aluminum (Al-100 wt%) and Al-Cu MMC. The results showed that excellent ultimate tensile strength, toughness, and electrical conductivity can be acquired simultaneously. The obtained ultimate tensile strength in the case of Al-100wt% (184.5 MPa) has improved two-fold than that of a typical commercially pure aluminum AA1016 (90 MPa). Similarly, the electrical conductivity of developed pure aluminum (88.87% IACS) is 1.4 times higher compared to AA1016 alloy (62% IACS). For Al-Cu MMC the copper is added in steps of 5 wt% (5%, 10%, 15%, and 20%). The maximum ultimate tensile strength (205.2 MPa) and the electrical conductivity (71.53% IACS) obtained for Al-10wt%Cu are higher compared to the AA1016 alloy. The present investigation suggests a novel processing route and opens up new research avenues in the field of solid-state materials processing.