Rafał Dańko

Prof. Rafał Dańko

orcid

Research Focus & Metrics

Academic Career Length

20Years (2007-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
6 December 2015 in Water, Air, & Soil Pollution
Verified
Journal Article
Open access
PDF file
MHMariusz Holtzer
Mariusz Holtzer
RDRafał Dańko
Rafał Dańko
Angelika KmitaAngelika Kmita
Angelika Kmita
Metalcasting involves having a molten metal poured in a hollow mould to produce metal objects. These moulds are generally made of sand and are chemically bonded, clay-bonded, or even unbounded. There are many binder systems used. Binders based on furfuryl resins constitute currently the highest fraction in the binders no-bake group. Moulding sand, after knocking out the cast, is partially reclaimed, and the remaining part, known as waste foundry sand is used or stored outside the foundry. In this case, the environment hazardous organic compounds and metals can be leached from the moulding sand, thus causing pollution of water and soil. Also during the casting moulds with molten metal, they emit pyrolysis gases containing many different compounds, often dangerous from the BTEX and PAH group, which has adverse impacts on the environment and workers. The article presents the results of research on the impact of the regenerate addition to the moulding sand matrix on emitted gases and the degree of threat to the environment due to leaching of hazardous components. Therefore, for the total assessment of the moulding sands harmfulness, it is necessary to perform investigations concerning the dangerous substances elution into the environment during their management and storage, as well as investigations concerning emissions of hazardous substances (especially from the BTEX and PAHs group) during moulds pouring, cooling, and casting knocking out. Both kinds of investigations indicated that reclaimed sand additions to moulding sands have significantly negative influence on the environment and working conditions.

1 October 2020 in Materials
Verified
Journal Article
Open access
PDF file
MHMariusz Holtzer
Mariusz Holtzer
RDRafał Dańko
Rafał Dańko
Angelika KmitaAngelika Kmita
Angelika Kmita
DDDARIUSZ DROŻYŃSKI
DARIUSZ DROŻYŃSKI
MKMichał Kubecki
Michał Kubecki
ARAgnieszka Roczniak
Agnieszka Roczniak
Increasingly strict regulations, as well as an increased public awareness, are forcing industry, including the foundry industry, to develop new binders for molding sands, which, while being more environmentally friendly, would simultaneously ensure a high quality of castings. Until recently, binders based on synthetic resins were considered to be such binders. However, more accurate investigations indicated that such molding sands subjected to high temperatures of liquid metal generated several harmful, even dangerous substances (carcinogenic and/or mutagenic) from the benzene, toluene, ethylbenzene and xylenes (BTEX) and polycyclic aromatic hydrocarbons groups (PAHs). An assessment of the most widely used molding sands technologies at present with organic binders (synthetic resins) from the no-bake group (furan no-bake and phenolic-ester no-bake) and their harmfulness to the environment and work conditions is presented in this paper. In the first stage of this research, gases (from the BTEX and PAHs groups) emitted when the tested molds were poured with liquid cast iron at 1350 °C were measured (according to the authors’ own method). The second stage consisted of measuring the emission of gases released by binders subjected to pyrolysis (the so-called flash pyrolysis), which simulated the effects occurring on the boundary: liquid metal/molding sand. The gases emitted from the tested binders indicated that, in both cases, the emission of harmful and dangerous substances (e.g., benzene) occurs, but, of the given binder systems, this emission was lower for the phenolic-ester no-bake binder. The obtained emission factors of BTEX substances show higher values for furan resin compared to formaldehyde resin; for example, the concentration of benzene per 1 kg of binder for furan no-bake (FNB) was 40,158 mg, while, for phenol-formaldehyde no-bake (PFNB), it was much lower, 30,911 mg. Thus, this system was more environmentally friendly.

18 August 2022 in Materials
Verified
Journal Article
Open access
PDF file
WKWojciech Kowalczyk
Wojciech Kowalczyk
RDRafał Dańko
Rafał Dańko
Marcin GórnyMarcin Górny
Marcin Górny
MKMagdalena Kawalec
Magdalena Kawalec
ABAndriy Burbelko
Andriy Burbelko
The paper presents the results of the research on the impact of process parameters of high-pressure, cold-chamber die casting of an industrial casting made of aluminium alloy on the casting properties assessed macroscopically by measuring the casting average density and microscopically through the characteristics of the casting microstructure. The analysis covers the influence of three selected velocity settings of the pressing plunger, which determine the filling time, and three values of the compression pressure setting characteristic of the third phase of the casting process. The cooling and solidification simulations of the casting were performed using the ProCAST software. During the simulation tests, the impact of the filling rate of the alloy into the die cavity on the cooling rate and the alloy solidification path at selected points were determined. The conducted research allowed linking the process parameters with the parameters of the casting structure with different wall thicknesses. Metallographic examinations of the castings were carried out using a light microscopy, SEM, and EDS analysis. The fraction of the phases α(Al), the size of dendritic cells, and the size of silicon particles, in the cross-sections of the castings with wall thickness of 3, 6, and 11 mm, respectively, were determined.

6 October 2015 in Archives of Foundry Engineering
Verified
Journal Article
Open access
PDF file
MHM. Holtzer
M. Holtzer
RDRafał Dańko
Rafał Dańko
JDJ. Dańko
J. Dańko
ZPZ. Pytel
Z. Pytel
The problem related to the management of post reclamation dusts generated in the reclamation process of waste moulding sands with organic binders is presented in the hereby paper. Waste materials generated in this process are products hazardous for the environment and should be utilised. The prototype stand for the utilisation of this dangerous material in its co-burning with coal was developed and patented in AGH in Krakow. The stand was installed in one of the domestic casting houses. As the utilisation result the transformed waste product is obtained and its management in the production of ceramic materials constitutes the subject of the presented publication.

1 April 2015 in Archives of Metallurgy and Materials
Verified
Journal Article
Open access
ABArtur Bobrowski
Artur Bobrowski
MHM. Holtzer
M. Holtzer
SŻS. Żymankowska-Kumon
S. Żymankowska-Kumon
RDRafał Dańko
Rafał Dańko
The harmfulness assessment of moulding sands with a geopolymer binder and a new hardener, in an aspect of the emission of substances from the BTEX group, was performed. Within the expedience project the new series of hardeners for the inorganic GEOPOL binder was developed. Before the introduction of the new system of moulding sands it was necessary to estimate their influence on the environment. To this aim the gasses emission from moulding sands subjected to the influence of liquid cast iron was tested with regard to the content of the gases from the BTEX group (benzene, toluene, ethylbenzene and xylenes). For the comparison the analogous investigations of the up to now applied moulding sands with the geopolymer binder, were performed. It was found that both systems of moulding sands binding emit similar amounts of gases, as well as similar amounts of substances from the BTEX group. Moulding sands with the GEOPOL binder are much more environmentally friendly than moulding sands with organic binders. The content of the BTEX group substances in gases emitted from moulding sands with the GEOPOL binder was approximately 10-times lower than in case of the moulding sands with organic binders

24 February 2016 in Arabian Journal of Geosciences
Verified
Journal Article
Open access
PDF file
RDRafał Dańko
Rafał Dańko
Jan JezierskiJan Jezierski
Jan Jezierski
MHMariusz Holtzer
Mariusz Holtzer
The paper presents the results of investigations of physical and chemical properties of after reclamation dust that is generated in the foundry industry. Universally applied mechanical reclamation processes of spent moulding sands generate large amounts of after-reclamation dusts containing mainly rubbed spent binding agents and quartz dusts. An amount of after-reclamation dusts—in dependence of the reclamation system efficiency and the reclaim dedusting system—can reach 5–10 % in relation to the total reclaimed spent moulding sand. After-reclamation dusts originated from spent moulding sands with different kinds of resins mostly belong to dangerous wastes, since they contain chemo-setting binders with dangerous substances removed in the reclamation process. None of the companies producing mechanical reclamation systems offers presently the complex technology and equipment for utilisation of after reclamation dusts, which would meet technical and economic expectations of foundry plants. The paper presents the results of research carried out at the Faculty of Foundry Engineering AGH UST in Cracow which aims on the determination of possibilities of using the post-reclamation dust generated during mechanical reclamation of used moulding sands with organic resins as a source of energy. Different dusts generated in the mechanical reclamation process of used organic sands, delivered from foundries, were tested to determine their chemical composition, granular characterisation and physicochemical properties. As a result of the investigations, possible ways to utilise the dusts are presented.