The PANI/Mesoporous MnO2 composites were prepared through a simple one step method and we introduced the KI-H2SO4 solution as the electrolyte of PANI/MnO2 composites creatively. The characterization of structure, morphology, and composition are obtained by X-ray diffraction, Fourier transform infrared spectroscopy, thermal gravity analysis, Raman spectra, and scanning electron microscope. The electrochemical performances were investigated by constant-current charge–discharge, the voltammetry curve, and alternating current (AC) impedance technique. The specific capacitance of composites is 1405 F/g, which is almost 10 times larger than MnO2 (158 F/g). We also find that the iodide concentration is closely related to the specific capacitance. Therefore, we explored the specific capacitance at different iodide concentration (0.05, 0.1, 0.2, 0.5, and 1 M), the results indicated that the specific capacitance reached a maximum value (1580 F/g) at 0.5 mol/L. Additionally, the PANI/Mesoporous MnO2 composites not only exhibited a good ratio discharge property (857 F/g) at high current density, but also revealed an excellent cycling stability after 500 cycles, which retained 90% of the original specific capacitance.
Mesoporous polyaniline-silica nanocomposites with a full interpenetrating structure for pseudocapacitors were synthesized via the vapor phase approach. The morphology and structure of the nanocomposites were deeply investigated by scanning electron microscopy, infrared spectroscopy, X-ray diffraction, thermal gravimetric analysis and nitrogen adsorption-desorption tests. The results present that the mesoporous nanocomposites possess a uniform particle morphology and full interpenetrating structure, leading to a continuous conductive polyaniline network with a large specific surface area. The electrochemical performances of the nanocomposites were tested in a mixed solution of sulfuric acid and potassium iodide. With the merits of a large specific surface area and suitable pore size distribution, the nanocomposite showed a large specific capacitance (1702.68 farad (F)/g) due to its higher utilization of the active material. This amazing value is almost three-times larger than that of bulk polyaniline when the same mass of active material was used.
Insufficient energy density and poor cyclic stability is still challenge for conductive polymer-based supercapacitor. Herein, high performance electrochemical system has been assembled by combining poly (3,4-ethylenedioxythiophene) (PEDOT):poly (styrene sulfonate) (PSS) redox electrode and potassium iodide redox electrolyte, which provide the maximum specific capacity of 51.3 mAh/g and the retention of specific capacity of 87.6% after 3000 cycles due to the synergic effect through a simultaneous redox reaction both in electrode and electrolyte, as well as the catalytic activity for reduction of triiodide of the PEDOT:PSS.
The cooperative effects between the PANI (polyaniline)/nano-NiO (nano nickel oxide) composite electrode material and redox electrolytes (potassium iodide, KI) for supercapacitor applications was firstly discussed in this article, providing a novel method to prepare nano-NiO by using β-cyelodextrin (β-CD) as the template agent. The experimental results revealed that the composite electrode processed a high specific capacitance (2122.75 F·g−1 at 0.1 A·g−1 in 0.05 M KI electrolyte solution), superior energy density (64.05 Wh·kg−1 at 0.2 A·g−1 in the two-electrode system) and excellent cycle performance (86% capacitance retention after 1000 cycles at 1.5 A·g−1). All those ultra-high electrical performances owe to the KI active material in the electrolyte and the PANI coated nano-NiO structure.
1 February 2014 in Progress in Natural Science: Materials International
A novel interpenetrating structural ultrafine polypropylene-silica nanocomposite particles were synthesized by a modified sol–gel approach in the presence of the melt polypropylene emulsion. A series of samples with different polypropylene content was prepared to investigate the unique characteristics of this original nanocomposite. The thermal gravimetric analysis and differential scanning calorimetry results showed that the nanocomposites had the interpenetrating structure and good thermal stability, and the crystallization behavior of polypropylene was confined by the silica matrix. The interpenetrating structure of nanocomposites was also suggested by the nitrogen adsorption–desorption measurement results. The scanning electronic microscope and transmission electron microscopy images indicated that the nanocomposites had irregular particle morphology. The nanoparticle tracking analysis results show that the mean size of the nanocomposites was around 160nm. According to the results obtained from different measurements, a reasonable formation mechanism was proposed