This paper explores the possibility of producing all-lignocellulosic fiberboards from Arundo donax L. as a source of lignocellulosic fibers with no synthetic binders. This raw material was steam exploded with a thermomechanical aqueous vapor process in a batch reactor. The Arundo donax raw material and its obtained pulp were characterized in terms of chemical composition and the results were compared to other lignocellulosic materials. The chemical composition of steam exploded Arundo fibers showed high cellulose and a moderate lignin content suggesting it was a good raw material for fiberboard production. The all-lignocellulosic fiberboards were produced on laboratory scale; using the steam exploded Arundo donax by means of a wet process. The effects of pressing pressure on physical and mechanical properties were evaluated and the conditions that optimize the responses were found. The analyzed properties were density (d); water absorption (WA); thickness swelling (TS); modulus of elasticity (MOE); modulus of rupture (MOR); and internal bond strength (IB). The tested levels of the pressing pressure range from 0.35 to 15 MPa. The optimum IB; MOE; MOR; WA and TS were 1.28 MPa, 7439 MPa, 40.4 MPa, 17.6% and 13.3%, respectively. The obtained fiberboards were of very good quality and more than satisfy the requirements of the relevant standard specifications.
This study presents an unexplored method to produce formaldehyde-free MDF. Steam exploded Arundo donax L. (STEX-AD) and untreated wood fibers (WF) were mixed at different mixing rates (0/100, 50/50, and 100/0, respectively) and two series of boards were manufactured, with 4 wt% of pMDI, based on dry fibers, and self-bonded. The mechanical and physical performance of the boards was analyzed as a function of the adhesive content and the density. The mechanical performance and dimensional stability were determined by following European standards. The material formulation and the density of the boards had a significant effect on both mechanical and physical properties. The boards made solely of STEX-AD were comparable to those made with pMDI, while the panels made of WF without adhesive were those that performed the worst. The STEX-AD showed the ability to reduce the TS for both pMDI-bonded and self-bonded boards, although leading to a high WA and a higher short-term absorption for the latter. The results presented show the feasibility of using STEX-AD in the manufacturing of self-bonded MDF and the improvement of dimensional stability. Nonetheless, further studies are needed especially to address the enhancement of the internal bond (IB).
The main objective of this work was to further analyze the optimization of the production factors of Arundo donax L. fiberboards obtained without adhesives. The production of boards derived from Arundo donax L. without added adhesives and with high mechanical performance has already been demonstrated. This present study explored a modification in the production process through a final curing thermal treatment (final heat treatment, FHT). Since pressing time is an influential factor in the production cost, it is expected that curing allows a reduction of this time. This study compared the results obtained by three panel-production alternatives: long pressing time (tp) without curing and long and short tp with FHT. Of the two factors analyzed, pressing pressure (Pp) was the most important production factor in both the modulus of elasticity (MOE) and modulus of rupture (MOR), while curing was the most important factor for the internal bond (IB). The study shows that a FHT facilitates the distribution of lignin and a possible improvement in the quantity and quality of bonds between lignin and cellulosic fibers. As a consequence, it improves the IB, produces boards with more homogeneous physical and mechanical properties and thereby makes them more hydrophobic. The curing thermal treatment allows high performance panels to be obtained in a manner which is more ecological, quicker, and cheaper.