The electromagnetic pollution problem is becoming increasingly serious due to the speedy advance of electronic communication devices. There are broad application prospects for the development of flexible, wearable composite films with high electromagnetic interference (EMI)-shielding performance. The MX@AC composite films were prepared from MXene, silver nanowires (AgNWs) and cellulose nanocrystals (CNCs) with a sandwich structure. Benefiting from the upper and lower frame structure formed by winding 1D AgNWs and CNC, the tensile strength of the MX@AC was improved to 35 MPa (12.5 wt% CNC content) from 4 MPa (0 wt% CNC content). The high conductivity of MXene and AgNWs resulted in the MX@AC composite film conductivity up to 90,670 S/m, EMI SE for 90 dB, as well as SSE/t up to 7797 dB cm2 g−1. And the MX@AC composite film was tested for practical application, showing that it can effectively isolate electromagnetic waves in practical application.
The purpose of this study was to investigate the effects of the microstructure and properties of Cu/Ni multilayer films prepared by magnetron sputtering and electroplating on the electrical explosion performance of the films. In this study, Cu/Ni multilayer films of the same thickness were prepared by electroplating (EP) and magnetron sputtering (MS), and their morphology and crystal structure were characterized by scanning electron microscope (SEM) and transmission electron microscope (TEM). XRD was used to observe the crystal structure and size of the samples. In addition, the Cu/Ni multilayer film was etched into the shape of a bridge, and the electric explosion phenomenon in the same discharge circuit of the multilayer foil obtained by the two preparation processes was tested by an electric explosion performance test system. The resistance–time curve and the energy–resistance curve during the electric explosion process were analyzed and calculated. The results showed that compared with the multilayer film prepared by the MS method, the crystal size of the multilayer film prepared by the EP method is smaller and the interface of Cu/Ni is clearer. In the electric explosion experiment, the MS samples had earlier burst times, larger peak resistances, smaller peak energies and higher ionization voltages. Through observation of the morphology of the samples after the electric explosion and combination with gas ionization theory, the internal influencing factors of the peak voltage and the relative resistance of the two samples were analyzed. The influence of the multilayer film mixing layer thickness on the sample energy conversion efficiency was analyzed by modeling the microstructure of the multilayer film exploding foil and electric heating. The results show that the thicker the mixing layer is, the more energy is distributed on the Ni, the faster the resistance increases, and the higher the energy conversion efficiency.
10 June 2020 in Propellants, Explosives, Pyrotechnics
The exploding foil initiator (EFI) system has been extensively used in ignition and detonation sequences and proved to be of high safety and reliability. Polyimide is considered the ideal flyer material for EFI due to its excellent performance, including thermal stability, outstanding mechanical properties, high radiation resistance, and excellent dielectric properties. In this study, we prepared the EFI based on a polyimide (ODPA-ODA) flyer, which is spin-coated and solidified on patterned copper film in situ. The electric explosion test shows that the prepared EFI has good working performance, and the 4000 V working voltage drove the flyer to reach a maximum velocity of 5096 m/s. The polyimide morphology and chemical structure after the electric explosion was observed by microscope, SEM, XPS, and FTIR, which showed that the polyimide flyer underwent thermal deformation and complex chemical reactions during an electric explosion. A large number of polyimide bonds broke to form new carbonyl compounds, and the opening of aromatic rings was accompanied by the formation of aliphatic hydrocarbon chains. The morphology and chemical structure analysis after the electric explosion test will lay a foundation for us to further understand the working principle and evolution process of polyimide (ODPA-ODA) flyer.