Over the past few years, various nanoparticle-supported precious metal-based catalysts have been investigated to reduce the emission of harmful substances from automobiles. Generally, precious metal nanoparticle-based exhaust gas catalysts are prepared using the impregnation method. However, these catalysts suffer from the low catalytic activity of the precious metal nanoparticles involved. Therefore, in this study, we developed a novel method for preparing highly efficient glass fiber-supported Pt nanoparticle catalysts. We uniformly deposited a single layer of platinum particles on the support surface using a chemically adsorbed monomolecular film. The octane combustion performance of the resulting catalyst was compared with that of a commercial catalyst. The precious metal loading ratio of the proposed catalyst was approximately seven times that of the commercial catalyst. Approximately one-twelfth of the mass of the proposed catalyst exhibited a performance comparable to that of the commercial catalyst. Thus, the synthesis method used herein can be used to reduce the weight, size, and manufacturing cost of exhaust gas purification devices used in cars.
TNTakahiro Kajitani, Osamu Tanaka, Yoshihiro Tange, and Hideaki MatsudaResearch Laboratory, Okura Industrial Co., Ltd., 1515 Nakatsu-cho, Marugame-city Kagawa, 763-8508 Japan Toshihiko Ooie, Tetsuo Yano, Masafumi Yoneda, and Munehide KatsumuraShikoku Nation
Takahiro Kajitani, Osamu Tanaka, Yoshihiro Tange, and Hideaki MatsudaResearch Laboratory, Okura Industrial Co., Ltd., 1515 Nakatsu-cho, Marugame-city Kagawa, 763-8508 Japan Toshihiko Ooie, Tetsuo Yano, Masafumi Yoneda, and Munehide KatsumuraShikoku Nation
+37
Thin films from six kinds of nonlinear optical nonpolymeric organic compounds were prepared by pulsed laser deposition (PLD) using a KrF excimer laser (248 nm) at various fluences up to 50 Changes in the chemical structure of the films with changes in fluence were studied. The experimental results show that for every compound at least minor decomposition has already started at the threshold fluence for deposition. More serious degradation occurs with increasing fluences, and little of the original chemical structure remains in films prepared by PLD at a fluence of 50