The effect of strain rate on the mechanical properties of AA5xxx series aluminum alloys containing solute Mg atoms (AA5005, AA5021, AA5082 and AA5182) and pure aluminum (A1070) was investigated within a wide strain rate range of 1.0 × 10−4 to 1.0 × 103 s−1 at room temperature. The A1070 exhibited a positive strain rate dependence of material strength at the investigated strain rates. However, the AA5xxx series aluminum alloys primarily exhibited the negative strain rate dependence of material strength and serration caused by the Portevin-Le Chatelier effect on the Mg content and strain rate. As a result of using the material constitutive equation for the negative strain rate dependence, it was found that the flow stress may change in the dynamic strain rate range. However, it was found that the strain rate dependence of material strength differed in the AA5082 and the AA5182 alloys. It would be caused by less solute Mg of the Al phase in the AA5182 alloy than in the AA5082 alloy, because more Mg2Si compounds precipitated on Mn bearing particles as precipitation sites in the AA5182 alloy.
The effect of strain rate on mechanical properties of Al-2.3wt.%Mg alloy (AA5021) and commercial pure aluminum (purity 99.7wt.%: A1070) was investigated at room temperature. The tensile tests were conducted at strain rates from 1.0×10−4 to 1.0×103 s−1. The universal testing machine was used for strain rate 1.0×10-4 to 1.0×10−1 s−1. For the strain rate 1.0×100 s-1, the servohydraulic testing machine, which was developed by our laboratory, was used. The impact strain rate 1.0×103 s−1 was obtained using the split Hopkinson pressure bar method. The pure aluminum showed positive strain rate dependence of material strength at the investigated strain rates. In contrast, the Al-2.3wt.%Mg alloy showed the negative strain rate dependence at strain rates from 1.0×10−4 to 1.0×100 s−1. However, Al-2.3wt.%Mg alloy showed the positive strain rate dependence at strain rates from 1.0×100 to 1.0×103 s−1. It was surmised that the effect of dislocation locking by the solute Mg atoms became negligible at strain rate of approximately 1.0×100 s−1. It was confirmed that material properties for the Al-Mg alloy at the strain rate of 1.0×100 s−1 were important, since the strain rate dependence changed negative to positive around this strain rate.
Serration phenomena, in which stress fluctuates in a saw-tooth shape, occur when a uniaxial test is performed on an aluminum alloy containing a solid solution of solute atoms. The appearance of the serrations is affected by the strain rate and temperature. Indentation tests enable the evaluation of a wide range of strain rates in a single test and are a convenient test method for evaluating serration phenomena. Previously, the serrations caused by indentation at room temperature were clarified using strain rate as an index. In this study, we considered ambient temperature as another possible influential factor. We clarify, through experimentation, the effect of temperature on the serration phenomenon caused by indentation. An Al–Zn–Mg–Cu alloy (7075 aluminum alloy) was used as the specimen. The aging phenomenon was controlled by varying the testing temperature of the solution-treated specimen. Furthermore, the material properties obtained by indentation were evaluated. By varying the testing temperature, the presence and amount of precipitation were controlled and the number of solute atoms was varied. Additionally, the diffusion of solute atoms was controlled by maintaining the displacement during indentations, and a favorable environment for the occurrence of serrations was induced. The obtained results reveal that the variations in the serrations formed in the loading curvature obtained via indentation are attributed to the extent of interaction between the solute atoms and the dislocations.