Acetabular hip joint components manufactured from gamma-sterilized ultra high molecular weight polyethylene (UHMWPE), gamma cross-linked UHMWPE, or polycarbonate-urethane (PCU) polymers were evaluated in a hip joint simulator, using cobalt alloy femoral components, for at least 5 million cycles. The volume of material losses due to wear was calculated for each type of sample, based upon mass loss measurements, every 500,000 cycles. The loss of material for the conventional UHMWPE was much higher than for the cross-linked UHMWPE, showing about a 70% reduction in wear due to cross-linking. The material loss for the PCU samples appears to have been at least 24% lower than for the cross-linked UHMWPE. Based upon these results, the PCU material seems to have potential for use as an alternative bearing material to UHMWPE for total hip replacement surgeries.
Modularity in total hip arthroplasty provides multiple benefits to the surgeon in restoring the appropriate alignment and position to a previously damaged hip joint. The vast majority of modern implants incorporate modularity into their design with some implants having multiple modular interfaces. There is the potential for failure at modular junctions because of fretting and crevice corrosion in combination with mechanical loading. This case report details the failure of an Emperion (Smith and Nephew, Memphis, TN) femoral stem in a 67-year-old male patient 6 years after total hip replacement. Analysis of the implant revealed mechanically assisted crevice corrosion that likely accelerated fatigue crack initiation in the hip stem. The benefits of modularity come with the potential drawback of a combination of fretting and crevice corrosion at the modular junction, which may accelerate fatigue, crack initiation and ultimately reduce the hip longevity.
5 March 2014 in Journal of Biomedical Materials Research Part B: Applied Biomaterials
Electron beam crosslinked ultra high molecular weight polyethylene (UHMWPE) 32 mm cups with cobalt alloy femoral heads were compared with gamma-irradiation sterilized 26 mm cups and zirconia ceramic heads in a hip wear simulator. The testing was performed for a total of ten million cycles with frequent stops for cleaning and measurement of mass losses due to wear. The results showed that the ceramic on UHMWPE bearing design exhibited higher early wear than the metal on highly crosslinked samples. Once a steady state wear rate was reached, the wear rates of the two types of hip bearing systems were similar with the ceramic on UHMPWE samples continuing to show a slightly higher rate of wear than the highly crosslinked samples. The wear rates of each of the tested systems appear to be consistent with the expectations for low rates of wear in improved hip replacement systems.