Solid-state hydrogen storage technology ensures a safer storage method, eliminating the risks of leaks, boiling losses, and explosions in commercial applications. Based on earlier findings, alloying LiH with silicon (Si) yields substantial storage capacity while lowering the energy needed for absorption and decomposition. Herein, the work explores using the derivative of bulk Si (i.e., porous silicon nanowires (PSiNWs)) after mechanical milling with LiH to improve the thermodynamic properties and uptake capacity. The PSiNWs are synthesized by Ag metal-assisted chemical etching of the bulk Si substrate. Nanopores on the nanowires enhance gas physisorption by overlapping attractive fields from opposing pore walls. The large surface area (∼450 m2 g−1) of the PSiNWs provides maximum active sites for hydrogen storage. The hydrogen storage capacity of the LiH–PSiNW alloy is evaluated through pressure composition isotherms at different temperatures (400–500 °C range) and ∼4 MPa charging pressure. The maximum observed capacity, ∼3.95 wt%, occurs at 400 °C. The thermodynamic analysis signifies the uniform absorption and desorption enthalpy after alloying LiH with PSiNWs. Hydrogen absorption and desorption enthalpies of ∼118 kJ mol−1 H2 and ∼115 kJ mol−1 H2 demonstrate a reduced energy requirement compared to individual LiH. The phase formation and variations before and after hydrogenation are studied by X-ray diffraction. This work investigates using Si nanostructures and light metal hydrides for enhanced hydrogen storage and cyclic functionalities, serving as both a storage material and catalyst.
Disproportionation and phase separation are big issues that occur under extreme pressure and temperature conditions during hydrogen compressor cycles, which makes metal hydrides inactive and reduces compression efficiency. It is important to identify boundary conditions to avoid such unwanted phase separation. However, no investigation related to this problem has been carried out so far. Thus we propose a method to investigate the critical temperature and pressure condition for the alloy degradation during the hydrogen compressor cycle. The V20Ti32Cr48 alloy was chosen as a model system for the purpose. The influence of two important parameters (i.e., hydrogen content and temperature) was investigated individually. The disproportionation of V20Ti32Cr48 alloy during the hydrogen compressor cycle test occurred at temperatures higher than 200 °C and 75% H2 content of the total capacity at the initial condition. A clear and obvious boundary condition between disproportionation and keeping the initial phase intact is defined herein. It can be treated as a general method for any hydrogen storage alloy to be utilized for hydrogen compressor efficiently and safely.
13 June 2023 in International Journal of Hydrogen Energy