Magnetron sputtered nickel oxide thin films deposited on the native oxide of crystalline n-Si(100) wafers are studied in dependence of the substrate deposition temperature (600 °C, 400 °C, 200 °C, and room temperature) using X-ray and synchrotron excited photoemission spectroscopy as well as cyclic-voltammetry under illumination. We show that the substrate temperature during nickel oxide sputtering governs the composition of the pristine NiOx film and the OER performance. Two dedicated nickel oxide species are found with Ni2+ corresponding to stoichiometric NiO while Ni3+ indicates an oxygen rich NiOx (x > 1) phase. With decreasing deposition temperature, the ratio of Ni3+/Ni2+ in the pristine NiOx film increases. Information depth dependent synchrotron related photoemission spectroscopy further suggests that oxygen rich NiOx is found on top of the surface and at the grain boundaries. The OER onset potential improves from 1.55 V to 1.1 V in correlation to an increasing Ni3+/Ni2+ ratio in the pristine NiOx film and an increasing emission from a nickel oxyhydroxide phase (h-NiOx) after photo-assisted cyclic-voltammetry in alkaline solution. Upon electrochemical treatment, a reconditioning process is observed with the formation of h-NiOx that consists of Ni(OH)2 and NiOOH, while NiOx disappears.
Using silicon in multijunction photocells leads to promising device structures for direct photoelectrochemical water splitting. In this regard, photoelectron spectra of silicon surfaces are used to investigate the energetic condition of contact formation. It is shown that the Fermi‐level position at the surface differs from the values expected from their bulk doping concentrations, indicating significant surface band bending which may limit the overall device efficiency. In this study, the influence of different surface preparation procedures for p‐ and n‐doped Si wafers on surface band bending is investigated. With the help of photoemission and X‐ray absorption spectroscopy, Si dangling bonds are identified as dominating defect centers at Si surfaces. These defects lead to an occupied defect band in the lower half and an unoccupied defect band in the upper half of the Si bandgap. However, partial oxidation of the defect centers causes a shift of defect bands, with only donor states remaining in the Si bandgap. Source‐induced photovoltages at cryogenic temperatures indicate that partial surface oxidation also decreases the recombination activity of these defect centers. It is shown that defect distribution, defect concentration, and source‐induced photovoltages need to be considered when analyzing Fermi‐level pinning at Si surfaces.
22 April 2019 in Journal of Vacuum Science & Technology A
A UHV-transferred Cu(In,Ga)Se2 (CIGSe) thin film prepared by a three-stage process on an Mo-coated float glass was successfully investigated by detailed UPS/XPS and directly compared with air-transferred and cyanide etched samples from the same batch. Besides the fact that the valence band maximum of the UHV-transferred sample is located 1.19 eV below the Fermi level, pointing to a widened bandgap and type inversion, almost no oxygen or sodium was detected on the surface. After air transfer, Na- and O-containing species were found on the CIGSe surface that could be only partially removed upon cyanide etching. The residual and very low Na1s signal is slightly shifted, which is attributed to a modified band bending at the grain boundaries with Ga-, In-, and Se-related oxides still present on the CIGSe surface after the etching process. Thickness analysis reveals that both the sodium containing surface layer (after air-transfer) and the oxygen containing termination layer (after cyanide etching) are restricted to a few monolayers only. Finally, the topmost CIGSe layer appears to be Cu-free due to the fact that no oxidized Cu was found after air exposure. In addition, the Cu core level does not follow the surface termination induced shift of the valence band after the KCN treatment, pinning its maximum 0.77 eV below the Fermi level. These findings are ascribed to a Cu(In,Ga)7Se11 surface as deduced from XPS core level analysis.