The aim of this work is to compare the corrosion resistance of nickel-base Alloy 625 (UNS N06625) produced by laser powder bed fusion with that obtained via conventional casting and hot working. Cyclic potentiodynamic polarization and potentiostatic tests were performed in order to evaluate the corrosion resistance of the differently manufactured alloys according to ASTM G5, and in NaCl 0.6 M solution at pH 7 and pH 3, at 40°C. The electrochemical characterization was carried out on the as-produced alloy and after annealing at 980°C for 32 minutes (according to ASTM B446). This heat treatment was also performed on the commercial hot worked alloy. Two surface conditions, namely as-built and polished surfaces, were investigated on the additive manufactured specimens. The alloy produced by laser powder bed fusion was not susceptible to pitting in the considered environments and had a good localized corrosion resistance, slightly higher than that of traditional wrought material. However, as predicted, the corrosion resistance of the as-built surfaces increased after mechanical polishing. The correlation between the corrosion performance and microstructure is also discussed.
CRUD (Chalk River Unidentified Deposit) forms in the water circuits of nuclear reactors due to corrosion of structural materials and the consequent release of species into the coolant. The deposition of CRUD is known to occur preferentially in regions of the primary circuit of pressurised water reactors (PWRs) where the water flow accelerates. In order to investigate this phenomenon, a micro-fluidic system, recreating plant conditions while using a simplified experimental set-up, was realised. A flow cell, comprising a stainless steel disc with a central micro-orifice, was used to create accelerated flow under representative operating conditions. By monitoring the pressure drop across the cell, the build-up rate (BUR) of CRUD within the micro-orifice was monitored in real time. By this setup, the conditions inducing deposition of CRUD under PWR conditions were emulated and CRUD deposition was induced in the accelerated flow region. Further effects associated with the presence of lithium hydroxide were investigated in real-time.
This paper describes some results selected from a larger program that was aimed at understanding the stress corrosion cracking (SCC) initiation of Type 304 stainless steel (UNS S30400) in high-temperature deaerated water. Out of a large number of statically loaded samples, only a small minority of the tested samples underwent SCC. The occurrence of SCC indicates a synergism between sensitization, ionic impurities (mainly chloride and sulfate), and/or superficial defects and cold work. In fact, none of the nonsensitized materials initiated cracking (within the time scale of the tests), while only three sensitized samples underwent extensive SCC. The crack morphology of the fractured sample was predominantly inter-granular with some transgranular regions. Transmission electron microscopic samples containing crack tips were, in most respect, in line with the literature: a magnetite/spinel duplex layer on the crack surfaces, a Cr-rich oxide at the crack tip, and Ni enrichment at the metal/oxide interface and oxidized deformation bands intercepting the crack flanks. Also, finger-like features protruding several hundreds of nanometers along the slip planes intersecting the intergranular crack were found on grain boundaries with a high degree of localized deformation. These results support the theory that cracking initiation and propagation might be associated with the formation of oxide on crystallographic planes inside the material.