For sodium‐ion batteries, two pressing issues concerning electrolytes are flammability and compatibility with hard carbon anode materials. Non‐flammable electrolytes that are sufficiently stable against hard carbon have—to the authors’ knowledge—previously only been obtained by either the use of high salt concentrations or additives. Herein, the authors present a simple, fluorine‐free, and flame‐retardant electrolyte which is compatible with hard carbon: 0.38 m sodium bis(oxalato)borate (NaBOB) in triethyl phosphate (TEP). A variety of techniques are employed to characterize the physical properties of the electrolyte, and to evaluate the electrochemical performance in full‐cell sodium‐ion batteries. The results reveal that the conductivity is sufficient for battery operation, no significant self‐discharge occurs, and a satisfactory passivation is enabled by the electrolyte. In fact, a mean discharge capacity of 107 ± 4 mAh g−1 is achieved at the 1005th cycle, using Prussian white cathodes and hard carbon anodes. Hence, the studied electrolyte is a promising candidate for use in sodium‐ion batteries.
In this study a number of work-piece variations were evaluated whilst limiting the cutting conditions. Eight wood species controlled at four moisture levels were machined along and across the wood grain. The tool used during cutting was designed to resemble a rip saw tooth with zero rake angle and narrow edge width. Each work-piece variation machined in the cutting tests was subjected to mechanical tests that evaluated bending properties across the grain and shear properties along the grain. The regression model establishes a relationship between the bending properties for cutting forces across the grain, as well as shear properties for cutting forces along the grain. F and R² values show that the elastic properties of the wood in bending and shear have less influence on the cutting forces when compared to the strength and toughness. Additionally, density is seen to have less influence on the cutting force along the grain. This is explained by the tool passing through an unquantifiable proportion of early and latewood fibers from the annual growth rings. Cutting across the grain, the tool is forced to machine through approximately the same proportion of earlywood and latewood fibres.
The articulating surfaces of four different sizes of unused pyrolytic carbon proximal interphalangeal prostheses (PIP) were evaluated though measuring several topographical parameters using a white light interferometer: average roughness (Sa); root mean-square roughness (Sq); skewness (Ssk); and kurtosis (Sku). The radii of the articulating surfaces were measured using a coordinate measuring machine, and were found to be: 2.5, 3.3, 4.2 and 4.7 mm for proximal, and 4.0, 5.1, 5.6 and 6.3 mm for medial components. ANOVA was used to assess the relationship between the component radii and each roughness parameter. Sa, Sq and Ssk correlated negatively with radius (p = 0.001, 0.001, 0.023), whilst Sku correlated positively with radius (p = 0.03). Ergo, the surfaces with the largest radii possessed the better topographical characteristics: low roughness, negative skewness, high kurtosis. Conversely, the surfaces with the smallest radii had poorer topographical characteristics.
19 May 2015 in Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine
Clinical results of the PyroCarbon proximal interphalangeal joint replacement are inconsistent with various complications reported. To address this, in vitro testing was conducted using finger joint simulators. Two PyroCarbon proximal interphalangeal prostheses were tested in a lubricant of dilute bovine serum to 5 × 106 cycles of flexion–extension (90°–30°) with dynamic forces of 10 N applied. At intervals of 3000 cycles testing ceased and a static load of 100 N was applied to simulate gripping. In addition, two ‘control’ prostheses were immersed alongside the test prostheses to account for lubricant absorption. Wear and roughness averages (Ra) were measured every 1 × 106 cycles. Minimal wear for all of the components was measured with a negligible increase in Ra for most of the components. One condyle of one component increased in Ra over the 5 × 106 cycles with a value above the recommended 50 nm. Unidirectional marks were visible on the condyle from micrographs, consistent with an abrasive wear mode.
A finger prosthesis consisting of a Cobalt-chromium (CoCr) proximal component and an Ultra-high-molecular-weight-polyethylene (UHMWPE) medial component (both mounted on hydroxyapatite coated stems) was evaluated to 5,000,000 cycles in an in vitro finger simulator. One “test” prosthesis was cycled through flexion-extension (90°–30°) with a dynamic load of 10 N, whilst immersed in a lubricant of dilute bovine serum. Additionally, a static load of 100 N was applied for 45 s every 3000 cycles to simulate a static gripping force. A second “control” prosthesis was immersed in the same lubricant to account for absorption. Gravimetric and Sa (3D roughness) measurements were taken at 1,000,000 cycle intervals. Micrographs and Sa values revealed negligible change to the CoCr surfaces after 5,000,000 cycles. The UHMWPE also exhibited no distinctive Sa trend, however the micrographs indicate that polishing occurred. Both the CoCr and UHMWPE test components progressively decreased in weight. The CoCr control component did not change in weight, whilst the UHMWPE component gained weight through absorption. To account for the disparity between surface and gravimetric results, the hydroxyapatite coatings were examined. Micrographs of the test stems revealed that the hydroxyapatite coating was partially removed, whilst the micrographs of the control stems exhibited a uniform coating.