In this paper, the influence of interface traps at the SiN/GaN interface and carbon-related buffer traps on GaN high electron mobility transistor (HEMT) on silicon substrate has been studied using high-frequency capacitance-voltage (HFCV) and quasi-static C-V (QSCV) measurement. The correlation between dynamic resistance degradation and trap density distribution subjected to pulse stress conditions has been examined. Deeper-level traps from the hole-emission process of the carbon-related buffer layer are activated by high drain voltage during off-state stress, and shallow-level traps at the SiN interface are enhanced by an increase in gate voltage during the on-state stress. 2-D device simulations have been carried out to probe the physical insight into the dynamic resistance degradation. Good agreement between experimental data and simulated results is obtained while taking into account shallow-level and deeper-level traps.
The gate charge change (ΔQg) of GaN-on-Si power devices subjected to different substrate biases has been investigated. On-wafer pulse-mode voltage stress measurement is examined to probe the physical insight of different trap mechanisms into Qg characteristics. Distinct injected electrons interacting with the buffer traps lead to a significant decrease (increase) in Qg under negative (positive) substrate bias. Different levels of degradation on ΔQgd to ΔQgs after stress under negative and positive substrate biases indicate uneven distribution of acceptor-like traps and uniform distribution of donor-like traps in the GaN buffer level. Using Arrhenius plots associated with the ΔQg shift, three dominant buffer traps with activation energies of EV + 0.542 eV, EC −0.604 eV, and EC −0.608 eV are extracted.
29 March 2021 in IEEE Transactions on Electron Devices
In this work, we present the substrate bias enhanced trap effects on time-dependent dielectric breakdown (TDDB) in GaN metal-insulator-semiconductor high electron mobility transistors (MIS-HEMTs) by experiment. Under different substrate biases, the shape parameter β and scale factor η of the Weibull distribution are extracted from the experimental data. A monotonical decrease in β from intrinsic breakdown to extrinsic breakdown relating to the hole-emission from the acceptor-like buffer traps with increased negative substrate biases has been observed, while η is increased at large positive substrate biases. This unexpected increase in η suggests that the donor-like buffer traps play an important role with a longer lifetime. The trap mechanisms, relating to percolation path establishment, are analyzed based on progressive breakdown (PBD). The capacitance-voltage characteristics are measured during each stress cycle confirming the hole fluence and electron injection in the gate-stack layer with different trap distributions under various substrate biases. Finally, 2-D device simulations are carried out to probe for physical insight into the traps on TDDB failure mechanisms.
21 March 2022 in IEEE Transactions on Device and Materials Reliability
The threshold voltage ( $\text{V}_{\mathrm{ th}}$ ) of p-GaN GaN-on-Si power devices has been examined under negative-bias temperature instability (NBTI) stress conditions, and the physical mechanisms are evaluated using 2D device simulation and experimental data. Three regimes of $\text{V}_{\mathrm{ th}}$ shift ( $\Delta \text{V}_{\mathrm{ th}}$ ) as a function of stress time and voltage magnitude at elevated temperatures have been investigated. Under the low gate stress condition, negative $\Delta \text{V}_{\mathrm{ th}}$ follows the power-law characteristics resulting from the electron de-trapping/injection process from the p-GaN region to the channel. Under the mid-stress condition, a bidirectional $\Delta \text{V}_{\mathrm{ th}}$ was recognized due to spill-over electrons into the p-GaN gate from the channel. At high gate stress, the hole accumulation at the interface between the Schottky contact and p-GaN is responsible for the negative $\Delta \text{V}_{\mathrm{ th}}$ .
30 August 2021 in IEEE Transactions on Device and Materials Reliability
This paper reports investigation of failure mechanisms of GaN-on-Si power device under electrostatic discharge (ESD) stress using on-wafer transmission-line pulse (TLP) testing. Hot-hole injections under the gate and filament formation in the buffer layer are examined by monitoring the threshold voltage ( $V_{th}$ ) and on-resistance ( $R_{on}$ ) subjected to a floating gate or an off-state gate voltage. Distinct and continued degradation has been observed after the ESD stress is removed indicating a slow de-trapping process due to deep-level buffer traps. Finally, 2D device simulation is used to probe the physical insight into failure mechanisms.
The Electrostatic Discharge (ESD) behavior of GaN-on-Si power devices is investigated using on-wafer transmission line pulse (TLP) and very fast transmission line pulse (VFTLP) measurements in different configurations. Under TLP measurement, two failure modes relating to electric field-and power- dependent mechanisms have been identified. Distinct ESD behavior with higher robustness characteristics has been observed under VFTLP measurement for the first time. Independent electric field failure mode with uniform thermal distribution has been recognized for the trigger voltage (V t1 ) and holding voltage (V h ) characteristics under VFTLP measurement.