The transition alumina (γ + δ)-Al2O3 was modified by intensive dehydroxylation, potassium-alkalization and hydrogenation, and examined for possible impacts of modification on surface (i.e. accessibility, chemical composition, functional groups and acid sites) and bulk properties by N2 sorptiometry, X-ray diffractometry, X-ray photoelectron spectroscopy, and infrared spectroscopy of adsorbed pyridine. Impacts on CO adsorption and resulting carboxy species on the surface and in the gas phase at 298–773 K, were subsequently examined by in-situ infrared spectroscopy of adsorbed CO at 298 K. Results communicated spectroscopic evidence for formation of various hydrogenocarbonate, formate, carbonate, carbonyl and end-on coordinated CO2 surface species, as well as CO2 gas phase species. Accordingly, it is concluded that: (i) surface hydroxylation of alumina (particularly the availability of basic OH-groups) enhances formation and thermal stability of hydrogenocarbonate and formate species, but hampers formation of carbonate species; (ii) surface alkalization with potassium ion additives disfavors appreciably formation of hydrogenocarbonate species, however enhances markedly formation of carbonate and formate species; and (iii) co-existence of H2 in the CO adsorptive atmosphere promotes both formation and thermal stability of surface formate species. Surface reaction pathways are proposed for the formation of the various surface and gas phase carboxy species at CO/Al2O3.
Si-doped alumina gels of nominal composition (Al2O3)0.88–(SiO2)0.12 have been synthesised in aqueous media and dried under different conditions in order to obtain xerogel (drying at 120 °C) or aerogel (supercritical CO2 drying) forms; after heating at 1200 °C for 5 h, the aerogel samples are more homogenous and retain a better specific surface area (>100 m2 g−1) than the xerogel samples.
Potassium-functionalised alumina (6 wt.% K–Al2O3) was obtained by calcination at 973 K of pure alumina particles (Al2O3) impregnated with an aqueous solution of K2CO3. Both Al2O3 and K–Al2O3 were, then, impregnated with aqueous RhCl3·3H2O, dried at 393 K, and in situ reduced in H2 atmosphere to obtain 1 wt.% Rh/Al2O3 and Rh/K–Al2O3 catalysts, respectively. Impacts of the potassium-functionalization on high-temperature behaviour of the Rh catalyst towards CO atmosphere were examined by (i) X-ray photoelectron spectroscopic analysis of the surface chemical composition, (ii) particle sizing of the Rh content by means of transmission electron microscopy, and (iii) in situ infrared spectroscopy of adsorbed CO. Results obtained showed the potassium-functionalization to suppress the CO-induced oxidative degradation of Rh0 metal particles into RhI, enrich the electronic density at Rh0 metal sites, and stabilize the Rh content against CO-assisted elimination at high temperatures. On the other hand, the presence of potassium was found not to affect the initially high dispersity of Rh0 metal particles on alumina despite the promoting effect on CO decomposition.
1 March 1999 in Journal de Chimie Physique et de Physico-Chimie Biologique