We present initial magnetic and structural characterization results of pressing barium hexaferrite pucks under the influence of a magnetic field using a custom-built uniaxial press. The press can be operated up to 500 pounds of load inside a 30 kG axially uniform magnetic field. We present details on the system specifications and operation procedures as well as results of pressing pucks in the system in a 0, 25, or 30 kG field. We find that the pucks pressed under a 25 or 30 kG field show similar properties but are significantly magnetically and crystallographically textured along the magnetic field direction used during pressing compared to the no-field pucks. For the 30 kG pressed pucks, we find a squareness value of 0.6, a saturation magnetization of 2.7 kG, a coercivity of 3.4 kOe, and a magnetic texture of 0.74. We also characterize the ferromagnetic resonance (FMR) behavior up to 66 GHz and find an anisotropy field of 21 kOe and zero-field FMR of 42 GHz.
4 October 2022 in Journal of Vacuum Science & Technology A
Plasma-enhanced atomic layer deposition (PEALD) enables the epitaxial growth of ultrathin indium nitride (InN) films at significantly reduced process temperatures and with greater control of layer thickness compared to other growth methods. However, the reliance on plasma-surface interactions increases the complexity of the growth process. A detailed understanding of the relationship between the plasma properties and the growth kinetics is therefore required to guide the tuning of growth parameters. We present an in situ investigation of the early-stage PEALD growth kinetics of epitaxial InN within three different plasma regimes using grazing incidence small-angle x-ray scattering (GISAXS). The GISAXS data are supported by diagnostic studies of the plasma species generation in the inductively coupled plasma source as a function of the relative concentrations of the nitrogen/argon gas mixture used in the growth process. The growth mode is found to be correlated to the production of nitrogen species in the plasma, with high concentrations of the atomic N species promoting Volmer–Weber growth (i.e., island growth) and low concentrations promoting Stranski–Krastanov growth (i.e., layer-plus-island growth). The critical thickness for island formation, island center-to-center distance, and island radius are found to increase with ion flux. Furthermore, the island center-to-center distance and areal density are observed to change only during plasma exposure and to continue changing with exposure even after the methylindium adlayer is believed to have fully reacted with the plasma. Our results demonstrate the potential to control the growth kinetics during PEALD of epitaxial films by intentionally accessing specific regimes of plasma species generation.
20 October 2019 in Journal of the American Ceramic Society