In this study, the thermal stability of a contact structure featuring hole-selective tungsten oxide (WOx) and aluminum deposited onto p-type crystalline silicon (c-Si/WOx/Al) was investigated using a combination of transmission line measurements (TLM) and in situ transmission electron microscopy (TEM) studies. The TEM images provide insight into why the charge carrier transport and recombination characteristics change as a function of temperature, particularly as the samples are annealed at temperatures above 500 °C. In the as-deposited state, a ≈ 2 nm silicon oxide (SiOx) interlayer forms at the c-Si/WOx interface and a ≈ 2–3 nm aluminum oxide (AlOx) interlayer at the WOx/Al interface. When annealing above 500 °C, Al diffusion begins, and above 600 °C complete intermixing of the SiOx, WOx, AlOx and Al layers occurs. This results in a large drop in the contact resistivity, but is the likely reason surface recombination increases at these high temperatures, since a c-Si/Al contact is basically being formed. This work provides some fundamental insight that can help in the development of WOx films as hole-selective rear contacts for p-type solar cells. Furthermore, this study demonstrates that in situ TEM can provide valuable information about thermal stability of transition metal oxides functioning as carrier-selective contacts in silicon solar cells.
In this study, the cross-section of electron-selective titanium oxide (TiO2) contacts for n-type crystalline silicon solar cells were investigated by transmission electron microscopy. It was revealed that the excellent cell efficiency of 21.6% obtained on n-type cells, featuring SiO2/TiO2/Al rear contacts and after forming gas annealing (FGA) at 350°C, is due to strong surface passivation of SiO2/TiO2 stack as well as low contact resistivity at the Si/SiO2/TiO2 heterojunction. This can be attributed to the transformation of amorphous TiO2 to a conducting TiO2−x phase. Conversely, the low efficiency (9.8%) obtained on cells featuring an a-Si:H/TiO2/Al rear contact is due to severe degradation of passivation of the a-Si:H upon FGA.