The laser hot-wire welding process was adopted to weld 7075 high-strength aluminum alloy. The influence laws of parameters on the weld formation were analyzed during laser hot-wire welding, and the microstructure characteristics and mechanical properties of welds were analyzed. The results showed that the parameters whose significance of influence on weld formation as ranked from high to low were laser power, current, gap width, welding speed and wire feeding rate. With the increase of wire temperature, the weld formation quality became better initially and then worse. Under the condition of optimized parameters, good weld formation could be obtained. The weld zone had a fine grain microstructure, and was in casting state consisted of dendritic crystal and equiaxed crystal. The heat affected zone mainly consisted of columnar crystal. The microhardness decreased gradually from base metal to heat affected zone then to weld zone. The tensile fracture of weld specimen occurred at the weld zone, and was in the ductile fracture state. The tensile strength of weld joint was 206 MPa and was 64.2% of base metal strength.
During Fuel Cell Vehicle (FCV) operation, the liquid water in gas diffusion media (GDM) prevents the reaction gas from reaching the reaction zone and lead to output power fluctuation and reduce the lifespan of FCV. In the present research, hydrophobicity gradient settings of micro-porous layer (MPL) and gas diffusion layer (GDL) are optimized to improve the water removal ability of GDM. Computational fluid dynamics (CFD) model is constructed for numerical simulations to analyze the fuel cell power output and the water content in the GDM with different hydrophobicity gradients. Experiments with different hydrophobicity gradients, which are specifically prepared with corresponding concentrations of polytetrafluoroethylene (PTFE) solutions, are conducted for validation of simulation results. It is shown that the positive hydrophobicity gradient of MPL and GDL provides a better capacity for water removal and oxygen transport. The contact angles of MPL and GDL are further optimized as 147.9°-138.6° by genetic algorithm integrated with the CFD simulations.
4 August 2021 in Metals and Materials International
In this study, an active noise control (ANC) algorithm based on fractional order with a variable step size is proposed to improve the convergence performance of an integer-order ANC algorithm and achieve noise cancellation of a train electric traction system fan. The algorithm optimized the convergence parameters by constructing a time-varying function related to the variation of an error signal to improve the convergence speed of the algorithm, and the introduction of fractional calculus in the algorithm to control the update iteration of the filter weight coefficients, which could improve the control accuracy of the algorithm and reduce the steady-state error. And we give proof of the convergence of the algorithm and compared the noise reduction effect of the system under different orders to obtain the optimal order. The algorithm is compared with other traditional algorithms, and it is proved that it is superior to traditional algorithms in terms of convergence speed, steady-state error, and error attenuation. The experimental results demonstrate that the algorithm exhibited a good noise reduction effect on the fan noise of the train electric traction system of 0–500 Hz and the average noise reduction was about 1.9–4.1 dB.
In order to clarify the effects of Sc modification on laser hot-wire welding performance of 7075 high strength aluminum alloys, the changing rules of weld formation, microstructure, element loss, mechanical performances and pores of weld joints were investigated during laser fusion welding, laser hot-wire welding and Sc-modified laser hot-wire welding. Comparing with laser fusion welding, the filler wire in laser hot-wire welding brought welding material and hot wire energy, resulting in better weld formation and sufficient fused weld joint. In laser hot-wire welding, tensile strength and elongation of weld joint were enhanced, element loss of weld joint was dramatically reduced and weld pore was reduced slightly. However, grains in fusion zone were relatively coarse, which caused lower microhardness in laser hot-wire welding. In Sc modified laser hot-wire welding, Sc modification led to smooth and continuous weld joint. During solidification of weld joints, Sc could combine with base metal to form Sc-containing alloy phase, which could lead to the formation of refined and equiaxed grains, thereby enhancing the yield strength of microstructure and increasing the microhardness, tensile strength and elongation of weld joint. In addition, Sc modification could increase the fluidity of molten pool, which thus promoted the escape of bubbles from the molten pool and hindered the formation of weld pores.