An attempt to degrade volatile organic compounds (VOCs) and sterilize air simultaneously is highly desirable to improve indoor air quality. With the help of deep ultraviolet (UVC) lighting, harmful bacteria that exists in the air can be destroyed. Thus, a new photocatalytic substance that can break down VOCs under UVC irradiation is required. Here, we demonstrate the photocatalytic activity of β-Ga2O3 nanostructures, synthesized via the solvothermal method for removing formaldehyde (HCHO) under deep ultraviolet irradiation. The Raman and XRD results indicated that as-synthesized nanostructures showed β-crystalline phase with a monoclinic structure. The photoluminescence spectrum exhibited a broad and strong green emission peak at 510 nm, which was likely attributed to a considerable amount of oxygen and gallium vacancies formed during the calcinating process. The photocatalytic efficiency for decomposing HCHO at room temperature under deep ultraviolet irradiation (278 nm) of the synthesized β-Ga2O3 nanoparticles is higher than that of the β-Ga2O3 nanorods. Both nanoparticles and nanorods obeyed the pseudo-first-order Langmuir-Hinshelwood kinetic model with a degradation rate constant of 0.057 and 0.033 min−1, corresponding to the efficiency of 82% and 62% in the formaldehyde removal, respectively.
The aggregation of zinc oxide nanoparticles leads to an increased absorbance in the ultraviolet-visible region by an induced light scattering effect. Herein, we demonstrate the inhibition of photoconversion activity in ZnO-graphene core-shell quantum dots (QD) (ZGQDs) agglomerated by 4-aminophenol (4-AP) used as a linker. The ZnO-graphene quantum dots (QD) aggregates (ZGAs) were synthesized using a facile solvothermal process. The ZGAs revealed an increased absorbance in the wavelengths between 350 and 750 nm as compared with the ZGQDs. Against expectation, the calculated average photoluminescence lifetime of ZGAs was 7.37 ns, which was 4.65 ns longer than that of ZGQDs and was mainly due to the high contribution of a slow (τ2, τ3) component by trapped carriers in the functional groups of graphene shells and 4-AP. The photoelectrochemical (PEC) cells and photodetectors (PDs) were fabricated to investigate the influence of ZGAs on the photoconversion activity. The photocurrent density of PEC cells with ZGAs was obtained as 0.04 mA/cm2 at 0.6 V, which was approximately 3.25 times lower than that of the ZGQDs. The rate constant value of the photodegradation value of rhodamine B was also decreased by around 1.4 times. Furthermore, the photoresponsivity of the PDs with ZGAs (1.54 μA·mW−1) was about 2.5 times as low as that of the PDs with ZGQDs (3.85 μA·mW−1). Consequently, it suggests that the device performances could be degraded by the inhibition phenomenon of the photoconversion activity in the ZGAs due to an increase of trap sites.