A self-cross-linking and biocompatible hydrogel has wide application potential in the field of tissue engineering. In this work, an easily available, biodegradable, and resilient hydrogel was prepared using a self-cross-linking method. This hydrogel was composed of N-2-hydroxypropyl trimethyl ammonium chloride chitosan (HACC) and oxidized sodium alginate (OSA). A stable and reversible cross-linking network was formed by the Schiff base self-cross-linked and hydrogen bonding. The addition of a shielding agent (NaCl) may weaken the intense electrostatic effect between HACC and OSA and solve the problem of flocculation caused by the rapid formation of ionic bonds, which provided an extended time for the Schiff base self-cross-linked reaction for forming a homogeneous hydrogel. Interestingly, the shortest time for the formation of the HACC/OSA hydrogel was within 74 s and the hydrogel had a uniform porous structure and enhanced mechanical properties. The HACC/OSA hydrogel withstood large compression deformation due to improved elasticity. What's more, this hydrogel possessed favorable swelling property, biodegradation, and water retention. The HACC/OSA hydrogels have great antibacterial properties against Staphylococcus aureus and Escherichia coli and demonstrated good cytocompatibility as well. The HACC/OSA hydrogels have a good sustained release effect on rhodamine (model drug). Thus, the obtained self-cross-linked HACC/OSA hydrogels in this study have potential applications in the field of biomedical carriers.
An ideal wound dressing for full-thickness wound regeneration should offer desirable biocompatibility, adequate mechanical properties, barrier function, and cellular regulation. Here, a bilayer scaffold resembling the hierarchical structure of human skin was developed using silk fibroin and sodium alginate. The upper membrane was prepared through casting and functioned as the epidermis, whereas the lower porous scaffold was prepared by freeze-drying and mimicked extracellular matrix structures. The membrane had nonporous structure, desirable mechanical properties, moderate hydrophilic surface, and suitable water vapor transmission rate, whereas the porous scaffold revealed 157.61 ± 41.67 µ m pore size, 86.10 ± 3.60% porosity, and capability of stimulating fibroblast proliferation. The combination of the two structures reinforced the tensile strength by five-fold and provided protection from wound dehydration. A suitable degradation rate reduced potential administration frequency. Furthermore, an in vivo rabbit full-thickness wound healing test demonstrated that the bilayer scaffold facilitated wound closure, granulation tissue formation, re-epithelialization and skin component transition towards normal skin by providing a moist wound environment, advancing the inflammation stage, and stimulating angiogenesis. Collectively, as an off-the-shelf and cell-free wound dressing with single topical administration, the bilayer scaffold is a promising wound dressing for full-thickness wound regeneration.