Polypropylene (PP) is regarded as the most promising candidate for eco-friendly high-voltage direct current (HVDC) cable insulation material due to its excellent thermal and electrical properties. In this paper, a block polypropylene (BPP) was selected as the matrix and blended with styrene-ethylene-butylene-styrene tri-block copolymer (SEBS) by melt blending. The thermal behavior, dynamic mechanical behavior, crystallization behavior, and mechanical and electrical properties of the BPP/SEBS blends were investigated. It was found that SEBS could efficiently improve the flexibility while maintaining the excellent heat resistance of PPB. Furthermore, adding an appropriate amount of SEBS had a positive effect on suppressing the space charge and increasing the breakdown field strength. For the BPP/SEBS blend containing 20 wt% SEBS, a desirable combination of thermal, mechanical, and electrical properties was achieved. This work may help pave the way for developing eco-friendly PP insulating material in HVDC cable applications.
Ethylene-vinyl acetate copolymer (EVA) was functionalized to varying degrees with acrylonitrile (AN) by melt grafting processes. Fourier transform infrared spectra (FT-IR) confirmed that AN was successfully grafted onto the EVA. High resistance meter, electronic universal testing machine, etc have studied the influencing factors of grafting process and the effect of grafting rate on oil resistance, mechanical properties and electrical properties. The results show that the optimal grafting process is that the dosage of AN is 8.0 wt%, the dosage of styrene (St) is 5.0 wt%, the dosage of Dilauroyl peroxide (LPO) is 0.4 wt% of the total amount of AN and St, and the grafting rate is 1.24%. With the increase of the amount of LPO and AN, the grafting rate first increased and then decreased. The grafting rate increases, so that the oil resistance, volume resistivity, and breakdown field strength of the grafted product are gradually increased. When the grafting rate is 1.24%, the volume resistivity is 1.63 × 1013 Ω·m, which is significantly improved compared with pure EVA, and the breakdown field strength is 23.26 kV mm−1, which is 12.3% higher than pure EVA.