In this present work, during high heat input welding of the weld metal, different types of Mn-depleted zones were achieved by different cooling rates. The effects of cooling rates on Mn-depleted zone formation and acicular ferrite (AF) transformation were analyzed. The Mn-depleted zone around the inclusions, as well as the interface concentration of Mn atoms, are found to be significantly different with different cooling rates. When the cooling rate is 10 °C/s, the interface concentration of Mn atoms around the inclusions is the lowest, the area of Mn-depleted zone is the smallest, and the proportion of AF in the weld metal is the highest. As the cooling rate decreases further, the interface concentration of Mn begins to rise, the area of the Mn-depleted zone gradually expands, and the proportion of AF decreases. However, when the cooling rate reaches 100 °C/s, only a very small amount of MnS precipitates, no Mn-depleted zone forms around the inclusions, and acicular ferrite cannot be produced effectively in the weld metal.
1 September 2014 in Advances in Mechanical Engineering
The in-situ observation of the phase transformation processes of weld metal during high-heat input welding were carried out by a high temperature laser confocal microscope. The influences of Ti content on the phase transformation process were investigated. It was found that the Ti inclusions could act as the nucleation sites for α→γ transformation during the heating stage of welding thermo cycle and inhibit the growth of austenite grains. The number of inclusions was increased with increasing Ti content. During the cooling stage of welding thermo cycle, the inclusions could induce the nucleation of acicular ferrites when the Ti content was below 0.078%. With increasing Ti content, more acicular ferrites collided with each other and restricted their further growth. When the Ti content was increased up to 0.115%, a proportion of Ti atoms were dissolved in the matrix, which increased the hardenability and thus generated the lath bainite microstructure instead of acicular ferrite.