The present investigation emphasizes studying the impact of the rotational tool speed and traverse speed on microstructure, mechanical properties, and corrosion behaviour of Al alloy AA6061 to Mg alloy AZ31B friction-stir welds. Results indicated that the use of the 1000 rpm rotation speed of the tool and 40 mm/min traverse speed led to increased weld strength and corrosion resistance. Owing to more heat generation, the surface of every friction stirs welded joint became rougher, and a keyhole can be observed. A maximum temperature of 311°C was observed for 1000 rpm of rotation speed and 40 mm/min of traverse speed, and a minimum temperature of 191°C was observed for 600 rpm of rotation speed and 80 mm/min of traverse speed. A minor tunnel defect can be partially observed at traverse speeds of 60 mm/min; the size of the tunnel defect becomes more prominent as the traverse speed rises to 80 mm/min. The joint with little or no defects was extracted at any rotational tool speed and a low traverse speed of 40 mm/min. The maximum value of UTS of 121 MPa was observed due to the better mechanical interlocking phenomena. It is approximately 41% of UTS of Al alloy AA6061 and 50% of UTS of Mg alloy AZ31B. Frictional heat, heavy plastic distortion, and grain refinement in the nugget zone are the reasons for the higher hardness value found mostly in weld nuggets. The FSW specimens indicate a primarily brittle type of failure, and a fracture of the cleavage type was seen with an excessive volume of intermetallic layer. Compared to both alloy side weld regions, the Mg alloy area weld zone was more corroded and had more cracks and gaps than the Al alloy side.
The evolution of microstructure and texture in three non-equiatomic CrMnFeCoNi high-entropy alloys (HEAs) with varying stacking fault energy (SFE) has been studied in up to 90% rolling reductions at both room and cryogenic temperature. All the HEAs deform by dislocation slip and additional mechanical twinning at intermediate and shear banding at high rolling strains. The microstructure is quite heterogeneous and, with strain, becomes highly fragmented. During rolling, a characteristic brass-type texture develops. Its strength increases with a decreasing SFE and the lowering of the rolling temperature. The texture evolution is discussed with regard to planar slip, mechanical twinning, and shear banding.
Developing soft magnetic materials with high saturation magnetization, low coercivity, and excellent mechanical properties remains a challenge. This study investigates the FeCoNiMn 0.25 Al 0.25 high-entropy alloy fabricated via vacuum arc melting. To analyze the effect of strain path, unidirectional and bidirectional cold rolling were applied with thickness reductions of 20%, 50%, and 90%. X-ray diffraction confirmed a face-centered cubic phase in cold rolling samples, while annealing at 900 °C led to a dual-phase structure (face-centered cubic + minor body-centered cubic). Deformation texture analysis revealed α-fiber components in unidirectional-cold rolling samples and normal direction-rotated brass components in bidirectional-cold rolling samples, with annealing twins influencing the final recrystallization texture. The M s values increased to ∼114.6 and 111.8 emu/gram, while H c decreased to ∼242.3 and 231.7 A/m for 90% cold rolling followed by annealing in unidirectional and bidirectional samples, respectively. Mechanical testing showed high hardness, yield strength, and tensile strength in cold rolling conditions, with improved plasticity after annealing. The unidirectional-annealed samples exhibited the best balance of magnetic and mechanical properties, making this high-entropy alloy a strong candidate for electrical machinery, transformers, magnetic shielding, and power generation applications.
21 July 2025 in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
Over the past decade, the utilization of additive manufacturing has gained momentum due to its near-net manufacturing capabilities, design adaptability, and expedited production capabilities. Wire-based additive manufacturing techniques offer promising avenues for the fabrication of metal parts with high deposition rates, low costs of materials and equipment, and strong structural integrity. However, existing wire-based, mostly gas tungsten arc welding (GTAW), and plasma-based techniques face many challenges due to process design complexities, expertise requirements, and higher costs. A twin-wire arc additive manufacturing (T-WAAM) system was developed using two gas metal arc welding (GMAW) systems because it was easier to weld, cheaper, and had higher deposition rates than the other wire-based techniques. Two GMAW systems were physically integrated, and torches were aligned 60° to each other for the wires to meet, melt, and form an alloy. The setup was calibrated with different parameters and was found to have a maximum error of 1% in distance, a decrease in time deviation with an increase in speed, and a decrease in percentage time deviation with distance. The process parameters were then optimized using the Box–Behnken and analysis of variance (ANOVA) techniques using two different wires of nickel and titanium. Using the optimal parameters, a sample was deposited and characterized for its microstructure, phases, phase transformation temperatures, and mechanical properties. The results displayed an excellent mixture with higher mechanical properties, confirming that the developed T-WAAM setup can be a competitive option compared to existing wire-based directed energy deposition techniques for developing alloys.