Addressing the issue that the Bayer process is not suitable for low-grade bauxite, carbochlorination was proposed to recover aluminum and silicon from low-grade bauxite. This study focused on the behavior of aluminum and silicon during the carbochlorination process of low-grade bauxite. The impact of various process parameters on the chlorination efficiency was investigated, and the chlorination mechanism and kinetics of aluminum and silicon chlorination in bauxite were analyzed and discussed. Under optimal experimental conditions, the chlorination efficiency of Al2O3 and SiO2 reached 94.93% and 86.32%, respectively. The carbochlorination of aluminum and silicon in bauxite adhered to a shrinking, unreacted core model governed by gas diffusion within the product layer. This process can be bifurcated into two stages. Additionally, calculations were conducted to determine the apparent activation energy and reaction order of the chlorination processes involving Al2O3 and SiO2. Examining the chlorination mechanism revealed that the bauxite carbochlorination encompasses transformations among various minerals. Notably, the aluminum component prefers to participate in the carbothermal chlorination reaction over silicon.
Aeration leaching was used to obtain synthetic rutile from a reduced ilmenite. The reduced ilmenite, obtained from the carbothermic reduction of ilmenite concentrate in a rotary kiln at about 1100 °C, contained 62.88% TiO2 and 28.93% Metallic iron. The particle size was about 200 μm and the size distribution was uniform. The effects of NH4Cl and HCl concentrations, stirring speed, and aeration leaching time on the extent of removal of metallic iron from the reduced ilmenite were studied at room temperature. The results revealed that aeration leaching is feasible at room temperature. When using the NH4Cl system, the metallic iron content was reduced to 1.98% in synthetic rutile, but the TiO2 content only reached 69.16%. Higher NH4Cl concentration did not improve the leaching. Using 2% NH4Cl with 3% HCl, we were able to upgrade the synthetic rutile to 75%, with a metallic iron content as low as 0.14% and a total iron content of about 4%. Synthetic rutile could be upgraded to about 90% using HCl solution alone. HCl and NH4Cl are both effective on the aeration leaching process. However, within the scope of this experiment, hydrochloric acid is more efficient in aeration leaching.
The technology for producing artificial rutile by the reduction-rusting method has the advantages of high product quality and less slag. A computational fluid dynamics (CFD) method is used to simulate the solid-liquid suspension and gas-liquid dispersion characteristics in the stirred corrosion reactor. The results show that the maximum volume fraction difference of the solid phase in the reactor with an upward-lifting impeller is 0.02, and for the downforce type, it is 0.04. When the stirring speed is increased from 100 rpm to 150 rpm, the radial dispersion area of the gas phase is increased; after the six-inclined-blade disk turbine is selected as the lower impeller, the proportion of bubbles with a diameter less than 0.004 m in the reactor is increased from 26% to 45%. The content of metallic iron in the product of the corrosion reaction is 1.67% in the stirred reactor with a six-inclined-blade disk turbine as the lower impeller.