The AA7075 composites reinforced with 3, 6, and 9 volume fractions (vol.%) of ZrB2 particles have been successfully fabricated using in situ fabrication method. In this technique, the inorganic salts K2ZrF6 and KBF4 were added to the molten aluminum and retained the melting at 900∘C to form the required vol.% of ZrB2 particles. The aluminum-reinforced metal matrix composites (MMCs) are commonly known as aluminum matrix composites (AMCs). This work carries the effects of various wire electrical discharge machining (WEDM) input process parameters like pulse-on-time ([ ]), pulse-off-time ([ ]), wire feed rate (WFR), and gap voltage (GV) on the output responses such as material removal rate (MRR), surface roughness (SR), and Kerf-width ([ ]) of the fabricated AA7075/(3, 6, and 9) vol.% ZrB2 in situ AMCs. Based on Taguchi’s L9 orthogonal array method, the design of experiments (DoE) was used to carry out the operations on the fabricated AMCs. The optimal level of process parameters was found by the main effects plot for signal-to-noise (S/N) ratio, contour plots, and the analysis of variance (ANOVA). The effect of these process parameters on MRR and SR was analyzed and it is found that the maximum MRR was attained in the optimal parametric combination of GV [ ][ ]V; [ ][ ][ ]s; [ ][ ][ ]s; WFR [ ][ ]mm/s; Reinforcement [ ] vol.%, and the minimum SR was attained in the optimal parametric combination of GV [ ][ ]V; [ ][ ][ ]s; [ ][ ][ ]s; WFR [ ][ ]mm/s; Reinforcement [ ] vol.%.
This study investigates the mechanical properties, water absorption and microstructural analysis of hybrid composites reinforced with Hemp fiber (HF) and Sisal fiber (SF) combined with Silicon Carbide (SiC) particles in epoxy composites. The fibers were treated with 5% NaOH solution for varying durations to enhance their properties. Composite laminates were fabricated using compression molding with different weight fractions of fibers (30 wt%) and SiC particles. The mechanical behaviour of the composites was evaluated through tensile, flexural, and water absorption tests following ASTM standards. The results shows that hybridization with hemp and sisal fibers improves the properties of epoxy composites, with increased hemp fiber content leading to enhanced mechanical performance.These included a tensile strength of 57.82 MPa, flexural strength of 94.7 MPa. The water absorption dipped in 120 hours of immersion in water, with the HFSF/SiC-5 showing the highest water absorption of 6%.The SEM images revealed a homogeneous distribution, fiber pullouts, voids of fibers and filler materials confirmed the presence in the composites.