Monitoring of human bodily motion requires wearable sensors that can detect position, velocity and acceleration. They should be cheap, lightweight, mechanically compliant and display reasonable sensitivity at high strains and strain rates. No reported material has simultaneously demonstrated all the above requirements. Here we describe a simple method to infuse liquid-exfoliated graphene into natural rubber to create conducting composites. These materials are excellent strain sensors displaying 104-fold increases in resistance and working at strains exceeding 800%. The sensitivity is reasonably high, with gauge factors of up to 35 observed. More importantly, these sensors can effectively track dynamic strain, working well at vibration frequencies of at least 160 Hz. At 60 Hz, we could monitor strains of at least 6% at strain rates exceeding 6000%/s. We have used these composites as bodily motion sensors, effectively monitoring joint and muscle motion as well and breathing and pulse.
25 January 2003 in Journal of the American Chemical Society
We have made electrical measurements on a system using carbon nanotubes as the dopant material. A semiconjugated, organic polymer was mixed with carbon nanotubes to form a wholly organic composite. Composite formation from low to high nanotube concentration increases the conductivity dramatically by ten orders of magnitude, indicative of percolative behavior. Effective mobilities were calculated from the space-charge regions of the current-voltage characteristics for the 0–8 % mass fractions. After an initial rise these were seen to fall from 1–8 % doping levels as predicted by theory. From the values for conductivity and mobility, an effective carrier density was calculated. This was seen to decrease between 0% and 1%, before rising steadily.